Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 12.1 µm/m-°C @Temperature 600 °C |
6.72 µin/in-°F @Temperature 1110 °F |
|
Outokumpu 4742 High Temperature Ferritic Stainless Steel Good scaling resistance and can be subjected to reducing sulphur environments without risk. Subject to 475°C embrittlement and grain coarsening at temperatures above 950°C. s-phase may form afte.. |
|||
CTE, linear | 12.1 µm/m-°C @Temperature 20.0 - 500 °C |
6.72 µin/in-°F @Temperature 68.0 - 932 °F |
|
Kennametal Stellite Stellite® 98M2 with P/M Processing Adhesive wear test data P/M 0.58 Typical applications include vane plugs, fuel metering pins, spacer bushings, ball bearing blanks, race bearing blanks, diesel engine exhaust, fluid valve seats, saw.. |
|||
CTE, linear | 12.1 µm/m-°C @Temperature 0.000 - 200 °C |
6.72 µin/in-°F @Temperature 32.0 - 392 °F |
|
Kennametal Stellite Stellite® STAR cast Applications: Vane plugs, fuel metering pins, spacer bushings, ball bearing blanks, race bearing blanks, diesel engine exhaust, fluid valve seats, saw cutter inserts, wear pads, pins, balls, hardfa.. |
|||
CTE, linear | 12.1 µm/m-°C @Temperature 20.0 - 500 °C |
6.72 µin/in-°F @Temperature 68.0 - 932 °F |
|
International Mold Steel DH31-EX Die Cast & Forging Steel DH31-EX is a hot working die steel with the best balance of strength and toughness showing the comparable softening resistance to SKD7 and twice hardenability as that of SKD61.Information provided b.. |
|||
CTE, linear | 12.1 µm/m-°C @Temperature 20.0 - 649 °C |
6.72 µin/in-°F @Temperature 68.0 - 1200 °F |
|
Latrobe Lescalloy® 410Cb High Strength Stainless Steel LESCALLOY 17-4 VAC-ARC steel is a precipitation hardening martensitic stainless steel. A wide range of mechanical properties is available via simple aging within a 900-1150°F (482-621°C) tempe.. |
|||
CTE, linear | 12.1 µm/m-°C @Temperature 20.0 - 300 °C |
6.72 µin/in-°F @Temperature 68.0 - 572 °F |
|
International Mold Steel DHA-World Die Cast & Forging Steel DHA-World is a high hardenability and high tough general use hot work die steel.Information provided by International Mold Steel |
|||
CTE, linear | 12.1 µm/m-°C @Temperature 25.0 - 200 °C |
6.72 µin/in-°F @Temperature 77.0 - 392 °F |
|
Haynes 263® alloy, cold rolled sheet, solution treated and aged Very good aged strength properties, excellent fabrication characteristics when annealed, excellent intermediate temperature tensile ductility, is not normally subject to strain age cracking, excelle.. |
|||
CTE, linear | 12.1 µm/m-°C @Temperature 25.0 - 100 °C |
6.72 µin/in-°F @Temperature 77.0 - 212 °F |
|
Haynes 282® Nickel Alloy Autogenously Welded Sheet Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la.. |
|||
CTE, linear | 12.1 µm/m-°C @Temperature 25.0 - 100 °C |
6.72 µin/in-°F @Temperature 77.0 - 212 °F |
|
Haynes 282® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) Plate Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la.. |
|||
CTE, linear | 12.1 µm/m-°C @Temperature 20.0 - 538 °C |
6.72 µin/in-°F @Temperature 68.0 - 1000 °F |
|
Latrobe Lescalloy® Jethete M-152 ESR 1.25 RD High Strength Stainless Steel LESCALLOY JETHETE M-152 ESR is a nitrogen bearing, hardenable 12% chromium stainless steel intended for various structural components requiring high strength and good oxidation resistance up to 800Â.. |
|||
CTE, linear | 12.1 µm/m-°C @Temperature 20.0 - 538 °C |
6.72 µin/in-°F @Temperature 68.0 - 1000 °F |
|
Latrobe Lescalloy® Jethete M-152 ESR 2.25" RD High Strength Stainless Steel LESCALLOY JETHETE M-152 ESR is a nitrogen bearing, hardenable 12% chromium stainless steel intended for various structural components requiring high strength and good oxidation resistance up to 800Â.. |
|||
CTE, linear | 12.1 µm/m-°C @Temperature 20.0 - 538 °C |
6.72 µin/in-°F @Temperature 68.0 - 1000 °F |
|
Latrobe Lescalloy® Jethete M-152 ESR 3" RD High Strength Stainless Steel LESCALLOY JETHETE M-152 ESR is a nitrogen bearing, hardenable 12% chromium stainless steel intended for various structural components requiring high strength and good oxidation resistance up to 800Â.. |
|||
CTE, linear | 12.1 µm/m-°C @Temperature 20.0 - 199 °C |
6.70 µin/in-°F @Temperature 68.0 - 390 °F |
|
EDRO #7 Shock Resistant S7 Tool Steel EDRO #7™ is a chromium-molybdenum steel characterized by: high toughness, good wear resistance, high impact resistance, good through hardening properties, good machinability, and good dimensional s.. |
|||
CTE, linear | 12.1 µm/m-°C @Temperature 21.1 - 649 °C |
6.70 µin/in-°F @Temperature 70.0 - 1200 °F |
|
Crucible Steel 422 Stainless Steel Crucible 422 is a hardenable martensitic stainless steel which is being widely used for high temperatures up to 1200°F. It has excellent creep-rupture properties in the range of 600/1200°F and is.. |
|||
CTE, linear | 12.1 µm/m-°C @Temperature 0.000 - 982 °C |
6.70 µin/in-°F @Temperature 32.0 - 1800 °F |
|
Crucible Steel 446 Chromium Steel Crucible 446 is a non-hardenable chromium steel which has the highest corrosion and heat resisting properties of the straight chromium steels. This grade is magnetic at all times. Information provi.. |
|||
CTE, linear | 12.1 µm/m-°C @Temperature 40.0 - 540 °C |
6.72 µin/in-°F @Temperature 104 - 1000 °F |
|
Crucible Steel CPM® Rex M4 HC(HS) Tool Steel CPM REX M4 HC(HS) is a high vanadium special purpose high speed steel exhibiting better wear resistance and toughness than M2 or M3 in cold work punches, die inserts and cutting applications involvi.. |
|||
CTE, linear | 12.1 µm/m-°C @Temperature 20.0 - 540 °C |
6.72 µin/in-°F @Temperature 68.0 - 1000 °F |
|
Crucible Steel CPM® Rex® 54® (HS) High Speed Steel CPM Rex 54 is a cobalt-bearing high speed steel designed to offer an improvement in the red hardness of the popular M4 grade, while maintaining wear properties equivalent to M4. CPM Rex 54 has a che.. |
|||
CTE, linear | 12.1 µm/m-°C @Temperature 21.1 - 93.3 °C |
6.70 µin/in-°F @Temperature 70.0 - 200 °F |
|
Crucible Steel CSM® 21 17Cr-4Ni Precipitation Hardening Stainless Steel CSM 21 is a precipitation hardening stainless mold steel, providing outstanding corrosion resistance and toughness, good polishability, and moderate wear resistance, combined with simple heat treatm.. |
|||
CTE, linear | 12.1 µm/m-°C @Temperature 21.1 - 538 °C |
6.72 µin/in-°F @Temperature 70.0 - 1000 °F |
|
Crucible Steel REX® M2 S 1.0C High Speed Steel, AISI M2 REX M2S (1.0C) is a sulfur-bearing high carbon version of the regular CRUCIBLE REX M2 high speed steel. The sulfur addition provides good grindability and an improvement in machinability of 25 to 35.. |
|||
CTE, linear | 12.1 µm/m-°C @Temperature 21.1 - 538 °C |
6.72 µin/in-°F @Temperature 70.0 - 1000 °F |
|
Crucible Steel REX® M2 S High Speed Steel REX M2 is a tungsten-molybdenum high speed steel which gives outstanding performance in all operations where a general purpose high speed steel is required. REX M2 has a wide hardening range, excell.. |
|||
CTE, linear | 12.1 µm/m-°C @Temperature 21.1 - 538 °C |
6.70 µin/in-°F @Temperature 70.0 - 1000 °F |
|
Crucible Steel REX® M3-1 High Speed Steel, AISI M3-1 REX M3-1 is a lower carbon, lower vanadium modification of M3-2 high speed steel. This lower alloy content results in better machining and grinding characteristics compared to M3-2, with a slight im.. |
|||
CTE, linear | 12.1 µm/m-°C @Temperature 21.1 - 427 °C |
6.70 µin/in-°F @Temperature 70.0 - 800 °F |
|
Crucible Steel WR-95 Tool Steel, AISI H10 Modified WR-95 is a modified H10, with cobalt added to improve its high temperature properties. It is an upgrade from H13 in applications requiring improved hot hardness or heat check resistance, at a slight.. |
|||
CTE, linear | 12.1 µm/m-°C @Temperature 0.000 - 316 °C |
6.70 µin/in-°F @Temperature 32.0 - 600 °F |
|
Crucible Steel 431 Chromium Steel Crucible 431 is a nickel bearing chromium steel which can be treated to exceptionally high physical properties. In the heat treated conditions, its corrosion resistance is superior to similar marten.. |
|||
CTE, linear | 12.1 µm/m-°C @Temperature 20.0 - 600 °C |
6.72 µin/in-°F @Temperature 68.0 - 1110 °F |
|
Bohler-Uddeholm BÖHLER M303 EXTRA Plastic Mold Steel BOHLER M303 EXTRA is a stainless martensitic chromium steel, offering excellent toughness, corrosion and wear resistance. It is characterized by improved machinability and polishability. BOHLER M303.. |
|||
CTE, linear | 12.1 µm/m-°C @Temperature <=649 °C |
6.72 µin/in-°F @Temperature <=1200 °F |
|
AK Steel 420HC Martensitic Stainless steel AK Steel 420 provides corrosion resistance similar to Type 410 martensitic stainless steel plus increased strength and hardness. It is magnetic in both the annealed and hardened conditions. Maximu.. |
|||
CTE, linear | 12.1 µm/m-°C @Temperature <=649 °C |
6.72 µin/in-°F @Temperature <=1200 °F |
|
AK Steel 420LC Martensitic Stainless steel AK Steel 420 provides corrosion resistance similar to Type 410 martensitic stainless steel plus increased strength and hardness. It is magnetic in both the annealed and hardened conditions. Maximu.. |
|||
CTE, linear | 12.1 µm/m-°C @Temperature 20.0 - 350 °C |
6.72 µin/in-°F @Temperature 68.0 - 662 °F |
|
Schmolz + Bickenbach Cryodur® 2990 Cold Work Die Steel Description: Newly developed ledeburitic cold-work steel with high hardness, good toughness and high tempering resistance combined with high wear resistance.Applications: Cutting and punching tools .. |
|||
CTE, linear | 12.1 µm/m-°C @Temperature 25.0 - 100 °C |
6.72 µin/in-°F @Temperature 77.0 - 212 °F |
|
Haynes 282® Nickel Alloy Plate, Solution Annealed and Age-Hardened Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and land-b.. |
|||
CTE, linear | 12.1 µm/m-°C @Temperature 20.0 - 538 °C |
6.72 µin/in-°F @Temperature 68.0 - 1000 °F |
|
Latrobe Lescalloy® Jethete M-152 ESR 6" RCS High Strength Stainless Steel LESCALLOY JETHETE M-152 ESR is a nitrogen bearing, hardenable 12% chromium stainless steel intended for various structural components requiring high strength and good oxidation resistance up to 800°.. |