Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 12.1 µm/m-°C @Temperature 21.1 - 93.3 °C |
6.70 µin/in-°F @Temperature 70.0 - 200 °F |
|
Schmolz + Bickenbach Thermodur® 2365 EFS Extra Fine Structure - Hot Work Die Steel Description: Thermodur® 2365 is an Extra Fine Structure (EFS) hot work tool steel developed for good high temperature strength and tempering resistance and Supplied in the annealed conditionChara.. |
|||
CTE, linear | 12.1 µm/m-°C @Temperature 20.0 - 199 °C |
6.70 µin/in-°F @Temperature 68.0 - 390 °F |
|
EDRO #7 Shock Resistant S7 Tool Steel EDRO #7™ is a chromium-molybdenum steel characterized by: high toughness, good wear resistance, high impact resistance, good through hardening properties, good machinability, and good dimensional s.. |
|||
CTE, linear | 12.1 µm/m-°C @Temperature 21.1 - 649 °C |
6.70 µin/in-°F @Temperature 70.0 - 1200 °F |
|
Crucible Steel 422 Stainless Steel Crucible 422 is a hardenable martensitic stainless steel which is being widely used for high temperatures up to 1200°F. It has excellent creep-rupture properties in the range of 600/1200°F and is.. |
|||
CTE, linear | 12.1 µm/m-°C @Temperature 0.000 - 982 °C |
6.70 µin/in-°F @Temperature 32.0 - 1800 °F |
|
Crucible Steel 446 Chromium Steel Crucible 446 is a non-hardenable chromium steel which has the highest corrosion and heat resisting properties of the straight chromium steels. This grade is magnetic at all times. Information provi.. |
|||
CTE, linear | 12.1 µm/m-°C @Temperature 20.0 - 427 °C |
6.70 µin/in-°F @Temperature 68.0 - 800 °F |
|
Crucible Steel CRUCIBLE A9 Tool Steel Crucible A9 is an air-hardening tool steel combining some of characteristics of the 5% chromium hot-work grades (such as H13) with the high attainable hardness and compressive yield strength of the .. |
|||
CTE, linear | 12.1 µm/m-°C @Temperature 21.1 - 93.3 °C |
6.70 µin/in-°F @Temperature 70.0 - 200 °F |
|
Crucible Steel CSM® 21 17Cr-4Ni Precipitation Hardening Stainless Steel CSM 21 is a precipitation hardening stainless mold steel, providing outstanding corrosion resistance and toughness, good polishability, and moderate wear resistance, combined with simple heat treatm.. |
|||
CTE, linear | 12.1 µm/m-°C @Temperature 21.1 - 427 °C |
6.70 µin/in-°F @Temperature 70.0 - 800 °F |
|
Crucible Steel HALCOMB® 425 Tool Steel, AISI H19 Halcomb 425 is designed for higher operating temperatures than H13, where wear resistance and heat check resistance are more critical than toughness. While H19 has excellent heat checking resistance.. |
|||
CTE, linear | 12.1 µm/m-°C @Temperature 21.1 - 316 °C |
6.70 µin/in-°F @Temperature 70.0 - 600 °F |
|
Crucible Steel HALGRAPH® Tool Steel, AISI O6 Halgraph is an oil-hardening graphitic tool steel with excellent non-deforming properties. Free graphite in its structure affords exceptional free-machining properties. The combination of graphite a.. |
|||
CTE, linear | 12.1 µm/m-°C @Temperature 21.1 - 538 °C |
6.70 µin/in-°F @Temperature 70.0 - 1000 °F |
|
Crucible Steel REX® M3-1 High Speed Steel, AISI M3-1 REX M3-1 is a lower carbon, lower vanadium modification of M3-2 high speed steel. This lower alloy content results in better machining and grinding characteristics compared to M3-2, with a slight im.. |
|||
CTE, linear | 12.1 µm/m-°C @Temperature 21.1 - 427 °C |
6.70 µin/in-°F @Temperature 70.0 - 800 °F |
|
Crucible Steel WR-95 Tool Steel, AISI H10 Modified WR-95 is a modified H10, with cobalt added to improve its high temperature properties. It is an upgrade from H13 in applications requiring improved hot hardness or heat check resistance, at a slight.. |
|||
CTE, linear | 12.1 µm/m-°C @Temperature 0.000 - 316 °C |
6.70 µin/in-°F @Temperature 32.0 - 600 °F |
|
Crucible Steel 431 Chromium Steel Crucible 431 is a nickel bearing chromium steel which can be treated to exceptionally high physical properties. In the heat treated conditions, its corrosion resistance is superior to similar marten.. |
|||
CTE, linear | 12.1 µm/m-°C @Temperature 20.0 - 400 °C |
6.70 µin/in-°F @Temperature 68.0 - 752 °F |
high temp. tempering, hardened to 62 HRC |
Bohler-Uddeholm AISI D2 Cold Work Tool Steel AISI D2 is a high-carbon, high-chromium tool steel alloyed with molybdenum and vanadiumAISI AD2 is characterized by: High wear resistance High compressive strength Good through-hardening properties.. |
|||
CTE, linear | 12.1 µm/m-°C @Temperature 199 °C |
6.70 µin/in-°F @Temperature 390 °F |
hardened to 57 HRC |
Bohler-Uddeholm COMPAX™ AISI S7 MOLD QUALITY Cold Work Steel Chromium-molybdenum alloyed steelA versatile S7 grade recommended for applications demanding a high degree of toughness and moderate wear resistance. Successfully used for heavy-duty punching and sh.. |
|||
CTE, linear | 12.1 µm/m-°C @Temperature 399 °C |
6.70 µin/in-°F @Temperature 750 °F |
hardened and tempered |
Bohler-Uddeholm UDDEHOLM VANADIS 23 (AISI M3:2) Hot Work Tool Steel Chromium-molybdenum-tungsten-vanadium alloyed PM steelVanadis 23 is a high speed powder metallurgical steel, recommended for low temperature die casting applications and warm forging applications wh.. |
|||
CTE, linear | 12.1 µm/m-°C @Temperature 399 °C |
6.70 µin/in-°F @Temperature 750 °F |
hardness of 60 HRC |
Bohler-Uddeholm UDDEHOLM VANADIS 6 Cold Work Tool Steel Description: Chromium-molybdenum-vanadium alloyed PM steel. Toolmaking with highly alloyed tool steel means that machining and heat treatment have to be considered more than with lower alloyed grade.. |
|||
CTE, linear | 12.1 µm/m-°C @Temperature 23.9 - 204 °C |
6.70 µin/in-°F @Temperature 75.0 - 400 °F |
|
Carlson GOC 276 Nickel-Molybdenum-Chromium General DescriptionCarlson Alloy GOC 276 is a nickel-molybdenum-chromium alloy exhibiting outstanding corrosion resistance over a wide range of service environments. This alloy is generally use in .. |