Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 6.70 - 7.40 µm/m-°C @Temperature 30.0 - 500 °C |
3.72 - 4.11 µin/in-°F @Temperature 86.0 - 932 °F |
|
ATI Allegheny Ludlum AL 42™ Electrical Alloy, UNS K94100 AL 42 alloy is used extensively in the manufacture of sealed beam automobile head lamps, in grommet and pin type glass-metal seals, and in integrated circuit lead frames. It is also the core metal .. |