Polymer Property : CTE, linear = 3.72 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 6.70 µm/m-°C

@Temperature 20.0 - 450 °C
3.72 µin/in-°F

@Temperature 68.0 - 842 °F
H.C. Starck WCu 90/10 Tungsten-Copper Composite Material
Description of Product: Tungsten-copper composite materials are produced by copper infiltration of porous sintered tungsten. They are available with different copper contents (10 - 30 %). A therm..
CTE, linear 6.70 µm/m-°C

@Temperature -30.0 - 70.0 °C
3.72 µin/in-°F

@Temperature -22.0 - 158 °F
Schott NG4 Neutral Density Filter
Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz..Similar glasses include NG3, NG1, NG5, NG9, NG10, NG11, NG 12
CTE, linear 6.70 µm/m-°C

@Temperature 20.0 - 300 °C
3.72 µin/in-°F

@Temperature 68.0 - 572 °F
Schott N-LASF43 Glass
Information Provided by SCHOTT North America, Inc.
CTE, linear 6.70 µm/m-°C

@Temperature -30.0 - 70.0 °C
3.72 µin/in-°F

@Temperature -22.0 - 158 °F
Schott N-SF2 Glass
Information Provided by SCHOTT North America, Inc.
CTE, linear 6.70 µm/m-°C

@Temperature 20.0 - 300 °C
3.72 µin/in-°F

@Temperature 68.0 - 572 °F
Schott N-SSK2 Glass
Information Provided by SCHOTT North America, Inc.
CTE, linear 6.70 µm/m-°C

@Temperature 20.0 - 300 °C
3.72 µin/in-°F

@Temperature 68.0 - 572 °F
Schott N-LAF33 Glass
Information Provided by SCHOTT North America, Inc.
CTE, linear 6.70 µm/m-°C

@Temperature 20.0 - 300 °C
3.72 µin/in-°F

@Temperature 68.0 - 572 °F
Schott N-LAK8 Glass
Information Provided by SCHOTT North America, Inc.
CTE, linear 6.70 µm/m-°C

@Temperature -30.0 - 70.0 °C
3.72 µin/in-°F

@Temperature -22.0 - 158 °F
Schott N-LASF31a Glass
Information Provided by SCHOTT North America, Inc.
CTE, linear 6.70 - 7.40 µm/m-°C

@Temperature 30.0 - 500 °C
3.72 - 4.11 µin/in-°F

@Temperature 86.0 - 932 °F
ATI Allegheny Ludlum AL 42™ Electrical Alloy, UNS K94100
AL 42 alloy is used extensively in the manufacture of sealed beam automobile head lamps, in grommet and pin type glass-metal seals, and in integrated circuit lead frames. It is also the core metal ..
CTE, linear 6.70 µm/m-°C

@Temperature 30.0 - 400 °C
3.72 µin/in-°F

@Temperature 86.0 - 752 °F
Ametek Tungsten-Copper Composites AWC 9010
Information supplied by Ametek Specialty Metal Products.The material is available as finished parts with the following maximum dimensions:Width: 6 inches (152 mm)Thickness: 0.150 inches (3.8 mm)Leng..