Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 6.70 µm/m-°C @Temperature 20.0 - 450 °C |
3.72 µin/in-°F @Temperature 68.0 - 842 °F |
|
H.C. Starck WCu 90/10 Tungsten-Copper Composite Material Description of Product: Tungsten-copper composite materials are produced by copper infiltration of porous sintered tungsten. They are available with different copper contents (10 - 30 %). A therm.. |
|||
CTE, linear | 6.70 µm/m-°C @Temperature -30.0 - 70.0 °C |
3.72 µin/in-°F @Temperature -22.0 - 158 °F |
|
Schott NG4 Neutral Density Filter Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz..Similar glasses include NG3, NG1, NG5, NG9, NG10, NG11, NG 12 |
|||
CTE, linear | 6.70 µm/m-°C @Temperature 20.0 - 300 °C |
3.72 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott N-LASF43 Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 6.70 µm/m-°C @Temperature -30.0 - 70.0 °C |
3.72 µin/in-°F @Temperature -22.0 - 158 °F |
|
Schott N-SF2 Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 6.70 µm/m-°C @Temperature 20.0 - 300 °C |
3.72 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott N-SSK2 Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 6.70 µm/m-°C @Temperature 20.0 - 300 °C |
3.72 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott N-LAF33 Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 6.70 µm/m-°C @Temperature 20.0 - 300 °C |
3.72 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott N-LAK8 Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 6.70 µm/m-°C @Temperature -30.0 - 70.0 °C |
3.72 µin/in-°F @Temperature -22.0 - 158 °F |
|
Schott N-LASF31a Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 6.70 - 7.40 µm/m-°C @Temperature 30.0 - 500 °C |
3.72 - 4.11 µin/in-°F @Temperature 86.0 - 932 °F |
|
ATI Allegheny Ludlum AL 42™ Electrical Alloy, UNS K94100 AL 42 alloy is used extensively in the manufacture of sealed beam automobile head lamps, in grommet and pin type glass-metal seals, and in integrated circuit lead frames. It is also the core metal .. |
|||
CTE, linear | 6.70 µm/m-°C @Temperature 30.0 - 400 °C |
3.72 µin/in-°F @Temperature 86.0 - 752 °F |
|
Ametek Tungsten-Copper Composites AWC 9010 Information supplied by Ametek Specialty Metal Products.The material is available as finished parts with the following maximum dimensions:Width: 6 inches (152 mm)Thickness: 0.150 inches (3.8 mm)Leng.. |