Thermal Properties Metric English Comments
CTE, linear 30.6 µm/m-°C

@Temperature >=149 °C
17.0 µin/in-°F

@Temperature >=300 °F
ASTM E228
Greene Tweed Arlon® 1555 PEEK, Carbon, Graphite Filled
Arlon® is a tough, high-temperature, semi-crystalline, thermoplastic presenting a unique combination of mechanical, thermal, chemical and electrical properties. Greene, Tweed uses several proprie..
CTE, linear 30.6 µm/m-°C

@Temperature >=149 °C
17.0 µin/in-°F

@Temperature >=300 °F
ASTM E228
Greene Tweed Arlon® 1263 PEEK, Carbon Filled
Arlon® is a tough, high-temperature, semi-crystalline, thermoplastic presenting a unique combination of mechanical, thermal, chemical and electrical properties. Greene, Tweed uses several proprie..