Greene Tweed Arlon® 1263 PEEK, Carbon Filled

Category Polymer , Thermoplastic , Polyketone , Polyetheretherketone (PEEK) , Polyetheretherketone, PEEK, Carbon Fiber Filled
Manufacturer Greene Tweed
Trade Name Arlon®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Greene Tweed Arlon® 1263 PEEK, Carbon Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Arlon® is a tough, high-temperature, semi-crystalline, thermoplastic presenting a unique combination of mechanical, thermal, chemical and electrical properties. Greene, Tweed uses several proprietary manufacturing and machining processes to ensure that Arlons properties consistently outperform the competition.Greene, Tweed offers several different Arlon materials, and all provide high tensile strength and elongation properties, excellent shear strength and creep resistance, outstanding fatigue resistance, broad chemical and radiation resistance, and no susceptibility to hydrolysis (steam/hot water). Our engineers work one on one with customers to find the right solution for each specific application.Information provided by Greene Tweed.
Physical Properties Metric English Comments
Specific Gravity 1.41 g/cc
1.41 g/cc
ASTM D792
Deformation 0.060 %
0.060 %
ASTM D621
Mechanical Properties Metric English Comments
Hardness, Rockwell M 108
108
ASTM D785
Hardness, Shore D 92
92
ASTM D2240
Tensile Strength at Break 230 MPa
33400 psi
ASTM D368
Elongation at Break 1.9 %
1.9 %
ASTM D638
Flexural Strength 347 MPa
50300 psi
ASTM D790
Flexural Modulus 19.0 GPa
2750 ksi
Flexural 0.5% Secant Modulus; ASTM D790
Compressive Yield Strength >= 4.14 MPa
>= 600 psi
Compressive Strength 262 MPa
38000 psi
ASTM D695
Shear Strength 95.8 MPa
13900 psi
Transverse; ASTM D732
120 MPa
17400 psi
Axial; ASTM D732
Secant Modulus 21.72 GPa
3150 ksi
Tensile 0.5% Secant Modulus; ASTM D638
Coefficient of Friction, Dynamic 0.18
0.18
PV=12600 psi-ft./min.; ASTM G77
Thermal Properties Metric English Comments
CTE, linear 12.6 µm/m-°C

@Temperature <=149 °C
7.00 µin/in-°F

@Temperature <=300 °F
ASTM E228
30.6 µm/m-°C

@Temperature >=149 °C
17.0 µin/in-°F

@Temperature >=300 °F
ASTM E228
Descriptive Properties Value Comments
Color Black