Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 5.70 µm/m-°C @Temperature 20.0 - 300 °C |
3.17 µin/in-°F @Temperature 68.0 - 572 °F |
|
H.C. Starck HPM 1750 Tungsten High Density Composite Description of Product: Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for furthe.. |
|||
CTE, linear | 5.70 µm/m-°C @Temperature 20.0 - 300 °C |
3.17 µin/in-°F @Temperature 68.0 - 572 °F |
|
H.C. Starck HPM 1750 Tungsten High Density Composite Sheet Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for further processing by the custo.. |
|||
CTE, linear | 5.70 µm/m-°C @Temperature 20.0 - 100 °C |
3.17 µin/in-°F @Temperature 68.0 - 212 °F |
|
H.C. Starck HPM 1751 Tungsten High Density Composite Description of Product: Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for furthe.. |
|||
CTE, linear | 5.70 µm/m-°C @Temperature 20.0 - 300 °C |
3.17 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott KZFSN5 Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 5.70 µm/m-°C @Temperature -30.0 - 70.0 °C |
3.17 µin/in-°F @Temperature -22.0 - 158 °F |
|
Schott N-LAF36 Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 5.70 µm/m-°C @Temperature -30.0 - 70.0 °C |
3.17 µin/in-°F @Temperature -22.0 - 158 °F |
|
Schott N-LAK10 Glass Information Provided by SCHOTT North America, Inc. |