Thermal Properties Metric English Comments
CTE, linear 215 - 250 µm/m-°C

@Temperature 25.0 - 300 °C
119 - 139 µin/in-°F

@Temperature 77.0 - 572 °F
ASTM D696
Polikim EFALON® T-100 Virgin PTFE
Applications: Gaskets, seals, O-rings, V-Rings, compression packings and similar sealing parts, Bushes, bearings and piston rings, Electrical insulators, Sliding supports, Conveyor belts, Coated tu..