Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 215 - 250 µm/m-°C @Temperature 25.0 - 300 °C |
119 - 139 µin/in-°F @Temperature 77.0 - 572 °F |
ASTM D696 |
Polikim EFALON® T-100 Virgin PTFE Applications: Gaskets, seals, O-rings, V-Rings, compression packings and similar sealing parts, Bushes, bearings and piston rings, Electrical insulators, Sliding supports, Conveyor belts, Coated tu.. |