Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 18.3 - 19.3 µm/m-°C

@Temperature 20.0 - 300 °C
10.2 - 10.7 µin/in-°F

@Temperature 68.0 - 572 °F
PEAK Werkstoff DISPAL S260 Aluminum Alloy, AlSi25Cu4Mg, Condition F
Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational..
CTE, linear 18.3 - 19.3 µm/m-°C

@Temperature 20.0 - 300 °C
10.2 - 10.7 µin/in-°F

@Temperature 68.0 - 572 °F
PEAK Werkstoff DISPAL S260 Aluminum Alloy, AlSi25Cu4Mg, Condition T7
Heat Treatment Condition T7 (Quenching in water at RT)Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allo..
CTE, linear 18.3 - 19.3 µm/m-°C

@Temperature 20.0 - 300 °C
10.2 - 10.7 µin/in-°F

@Temperature 68.0 - 572 °F
PEAK Werkstoff DISPAL S260 Aluminum Alloy, AlSi25Cu4Mg, Condition T6
Heat Treatment Condition T6 (Quenching in water at RT)Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allo..