Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 18.8 µm/m-°C @Temperature 500 °C |
10.4 µin/in-°F @Temperature 932 °F |
|
Outokumpu 4841 High Temperature Austenitic Stainless Steel Variant of 1.4845 with an increased silicon content which enhances the steel's resistance to oxidation/corrosion but has also made it more susceptible to embrittlement.Applications: Heat and creep r.. |