QuesTek® Innovations Ferrium® M54™ Ultrahigh-strength Steel for Structural Applications
Description: Ferrium® M54™ is an ultra high-strength steel for structural applications. Ferrium® M54™ was designed to provide mechanical properties equal to, or better than ultrahigh-strength st..
CTE, linear 11.1 µm/m-°C

@Temperature 20.0 - 500 °C
6.17 µin/in-°F

@Temperature 68.0 - 932 °F
Kennametal Stellite Delcrome® 93
Information provided by Deloro Stellite, Inc. Typical data, not guaranteed as a maximum or minimum. Highly alloyed white cast iron, abrasion resistant. Carbides in a martensitic matrix offer high..
CTE, linear 11.1 µm/m-°C

@Temperature 20.0 - 200 °C
6.17 µin/in-°F

@Temperature 68.0 - 392 °F
Kennametal Stellite Stellite® 98M2 cast
Adhesive wear test data P/M 0.58 Typical applications include vane plugs, fuel metering pins, spacer bushings, ball bearing blanks, race bearing blanks, diesel engine exhaust, fluid valve seats, saw..
CTE, linear 11.1 µm/m-°C

@Temperature 20.0 - 200 °C
6.17 µin/in-°F

@Temperature 68.0 - 392 °F
Kennametal Stellite Stellite® 98M2 with P/M Processing
Adhesive wear test data P/M 0.58 Typical applications include vane plugs, fuel metering pins, spacer bushings, ball bearing blanks, race bearing blanks, diesel engine exhaust, fluid valve seats, saw..
CTE, linear 11.1 µm/m-°C

@Temperature 20.0 - 100 °C
6.17 µin/in-°F

@Temperature 68.0 - 212 °F
International Mold Steel Daido DRM3 Matrix High-Speed Steel
This conventional grade MH88 has been improved to DRM3. High hardness and tough DRM3 with excellent hardenability is suitable for high precision cold working tools.Information provided by Internatio..
CTE, linear 11.1 µm/m-°C

@Temperature 20.0 - 200 °C
6.17 µin/in-°F

@Temperature 68.0 - 392 °F
Industeel CLC 1.2316 Prehardened (300HB) and Corrosion Resistant Mold Steel
Description: CLC 1.2316 is a 16%Cr 1% Mo with improved corrosion resistance properties, thanks to the chromium/molybdenum additions. The high cleanliness/homogeneity of the steel makes it specially ..
CTE, linear 11.1 µm/m-°C

@Temperature 20.0 - 200 °C
6.17 µin/in-°F

@Temperature 68.0 - 392 °F
Industeel CLC 1.2316S Prehardened Mold Steel (300HB) with Improved Machinability
Description: CLC 1.2316 S grade is a 16%Cr 1%Mo mold steel with improved corrosion resistance properties, thanks to the chromium and molybdenum additions. Furthermore specific sulfur additions are c..
CTE, linear 11.1 µm/m-°C

@Temperature 25.0 - 100 °C
6.17 µin/in-°F

@Temperature 77.0 - 212 °F
Haynes 263® alloy, cold rolled sheet, solution treated and aged
Very good aged strength properties, excellent fabrication characteristics when annealed, excellent intermediate temperature tensile ductility, is not normally subject to strain age cracking, excelle..
CTE, linear 11.1 µm/m-°C

@Temperature 20.0 - 300 °C
6.17 µin/in-°F

@Temperature 68.0 - 572 °F
Schott P-SF8 Glass
Suitable for precision moldingInformation Provided by SCHOTT North America, Inc.
CTE, linear 11.1 µm/m-°C

@Temperature 20.0 - 100 °C
6.17 µin/in-°F

@Temperature 68.0 - 212 °F
DIN EN 821-1
CeramTec MZ 111 HIP Zirconia, ZrO2-Y2O3
MZ 111 HIP is a yttria-stabilized tetragonal zirconia ceramic.
CTE, linear 11.1 µm/m-°C

@Temperature 20.0 - 100 °C
6.17 µin/in-°F

@Temperature 68.0 - 212 °F
DIN EN 821-1
CeramTec MZ 111 Zirconia, ZrO2-Y2O3
MZ 111 is a yttria-stabilized tetragonal zirconia used in dental applications.
CTE, linear 11.1 µm/m-°C

@Temperature 20.0 - 100 °C
6.17 µin/in-°F

@Temperature 68.0 - 212 °F
DIN EN 821-1
CeramTec MZ 429 Zirconia, ZrO2-Y2O3
MZ 429 is a yttria-stabilized zirconia ceramic.
CTE, linear 11.1 µm/m-°C

@Temperature 21.0 - 260 °C
6.17 µin/in-°F

@Temperature 69.8 - 500 °F
Crucible Steel CPM® 10V® (AISI A11) Tool Steel
CPM 10V was the first in the family of high vanadium tool steels made by the Crucible Particle Metallurgy process. Crucible engineers optimized the vanadium content to provide superior wear resistan..
CTE, linear 11.1 µm/m-°C

@Temperature 21.0 - 260 °C
6.17 µin/in-°F

@Temperature 69.8 - 500 °F
Crucible Steel CPM® 15V® Tool Steel
CPM 15V is intended for applications requiring exceptional wear resistance. It has more vanadium carbides in its microstructure than CPM 10V and provides more wear resistance and longer tool life in..
CTE, linear 11.1 µm/m-°C

@Temperature 21.1 - 204 °C
6.14 µin/in-°F

@Temperature 70.0 - 400 °F
Crucible Steel CSM® S60V (440V) Tool Steel, AISI 440C Modified
CPM S60V is a unique tool steel made by the Crucible Particle Metallurgy process. It is designed from a 440C stainless base analysis with added high carbon and vanadium for exceptionally good wear r..
CTE, linear 11.1 µm/m-°C

@Temperature 20.0 - 260 °C
6.17 µin/in-°F

@Temperature 68.0 - 500 °F
Bohler-Uddeholm BÖHLER K294 MICROCLEAN AISI A11 Powder Metal Tool Steel
Properties: Powder-metallurgical produced cold work tool steel with extremely high wear resistance, good toughness and high compressive strength. The latest generation of powder metal technology ena..
CTE, linear 11.1 µm/m-°C

@Temperature 20.0 - 300 °C
6.17 µin/in-°F

@Temperature 68.0 - 572 °F
Bohler-Uddeholm BÖHLER M303 EXTRA Plastic Mold Steel
BOHLER M303 EXTRA is a stainless martensitic chromium steel, offering excellent toughness, corrosion and wear resistance. It is characterized by improved machinability and polishability. BOHLER M303..
CTE, linear 11.1 µm/m-°C

@Temperature 20.0 - 200 °C
6.17 µin/in-°F

@Temperature 68.0 - 392 °F
Bohler-Uddeholm UDDEHOLM MIRRAX ESR Plastic Mold Steel
Uddeholm Mirrax ESR is specially developed and adapted for larger molds that require corrosion resistance and/or high surface finish.It is characterized by:High hardenability for consistent properti..
CTE, linear 11.1 µm/m-°C

@Temperature 20.0 - 200 °C
6.17 µin/in-°F

@Temperature 68.0 - 392 °F
Bohler-Uddeholm UDDEHOLM Vancron 40 nitrided powder tool steel
Description: Uddeholm Vancron 40 is a nitrided powder tool steel, which means that a “surface coating” is already integrated into the finished tooling material. The result is a tool surface with v..
CTE, linear 11.1 µm/m-°C

@Temperature -17.8 - 100 °C
6.17 µin/in-°F

@Temperature 0.000 - 212 °F
American Utility Metals Cromgard® Stainless Steel
Cromgard is a low cost stainless steel, which is able to provide benefits of good weldability and formability, making it capable of fabrication by conventional techniques. It provides the benefits o..
CTE, linear 11.1 µm/m-°C

@Temperature 20.0 - 600 °C
6.17 µin/in-°F

@Temperature 68.0 - 1110 °F
for the hardened and tempered condition
Assab Steels ASP 60 Cold Work Steel
ASP 60 is a W-Mo-V-Co alloyed PM high speed steel characterized by:Highest wear resistanceMaximum compressive strengthGood through hardening propertiesGood toughnessGood dimensional stability on hea..
CTE, linear 11.1 µm/m-°C

@Temperature 20.0 - 100 °C
6.17 µin/in-°F

@Temperature 68.0 - 212 °F
Bohler-Uddeholm BÖHLER W360 ISOBLOC® Hot Work Tool Steel
BÖHLER W360 ISOBLOC was developed as a tool steel for dies and punches in warm and hot forging. The steel can be used for a variety of applications where hardness and toughness are required. Prope..
CTE, linear 11.1 µm/m-°C

@Temperature 20.0 - 200 °C
6.17 µin/in-°F

@Temperature 68.0 - 392 °F
Assab Steels ASP 23 Cold Work Steel
ASP 23 is a chromium-molybdenum-tungsten-vanadium alloyed high speed steel which is characterized by:High wear resistance (abrasive profile)High compressive strengthVery good through-hardening prope..
CTE, linear 11.1 µm/m-°C

@Temperature 20.0 - 300 °C
6.17 µin/in-°F

@Temperature 68.0 - 572 °F
Schmolz + Bickenbach Formadur® 2316/2316 ESR Plastic Mold Steel
Increased corrosion resistance in comparison to Formadur 2083, good polishability. Usually this grade is supplied quenched and tempered to 300 HBApplications: Molds for processing plastics with corr..