Polymer Property : CTE, linear, Transverse to Flow = 78.0 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 60.0 - 78.0 µm/m-°C
33.3 - 43.3 µin/in-°F
Average value: 69.2 µm/m-°C Grade Count:6
Overview of materials for PCTG Copolyester
This property data is a summary of similar materials in the MatWeb database for the category "PCTG Copolyester". Each property range of values reported is minimum and maximum values of appropriate M..