Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 60.0 - 78.0 µm/m-°C | 33.3 - 43.3 µin/in-°F | Average value: 69.2 µm/m-°C Grade Count:6 |
Overview of materials for PCTG Copolyester This property data is a summary of similar materials in the MatWeb database for the category "PCTG Copolyester". Each property range of values reported is minimum and maximum values of appropriate M.. |