Polymer Property : CTE, linear, Transverse to Flow = 57.2 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 103 µm/m-°C

@Temperature -40.0 - 40.0 °C
57.2 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP LUBRILOY R2000 PA 66
LNP* LUBRILOY* R2000 is a compound based on Nylon 66 resin containing Proprietary Lubricant. Added feature of this material is: Wear Resistant.
CTE, linear, Transverse to Flow 103 µm/m-°C

@Temperature -40.0 - 40.0 °C
57.2 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP LUBRILOY R2000 PA 66 (Asia Pacific)
LNP* Lubriloy* R2000 is a compound based on Nylon 66 resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated.
CTE, linear, Transverse to Flow 103 µm/m-°C

@Temperature -40.0 - 40.0 °C
57.2 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP LUBRILOY R2000 PA 66 (Europe-Africa-Middle East)
LNP* Lubriloy* R2000 is a compound based on Nylon 66 resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated.
CTE, linear, Transverse to Flow 103 µm/m-°C

@Temperature 20.0 °C
57.2 µin/in-°F

@Temperature 68.0 °F
ASTM E381
Solvay Specialty Polymers Mindel® S-1000 Modified Polysulfone  (discontinued **)
This product line was acquired by Solvay Advanced Polymers from BP Amoco in November 2001.
CTE, linear, Transverse to Flow 103 µm/m-°C

@Temperature -40.0 - 40.0 °C
57.2 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics NORYL PX1005X PPE+PS
PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. UL94 V0/5VA rated. UL746C F1. Excelent dielectric strength. Suitable for E/E market in indoor/outdoor applications.
CTE, linear, Transverse to Flow 103 µm/m-°C

@Temperature -30.0 - 30.0 °C
57.2 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D 696
SABIC Innovative Plastics LNP Stat-kon MDM40 PP
LNP* Stat-Kon* MDM40 is a compound based on Polypropylene resin containing Mica and Carbon. Characteristics are Statically Conductive.This data was supplied by SABIC-IP for the Americas region.