Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 34.0 - 2980 µm/m-°C
18.9 - 1660 µin/in-°F
Average value: 473 µm/m-°C Grade Count:7
Overview of materials for Polyphenylene Sulfide (PPS) with 30% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 30% Glass Fiber Filler". Specific grades with glass content between 25%..