Polymer Property : CTE, linear, Transverse to Flow = 162 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 162 µm/m-°C

@Temperature 23.0 - 60.0 °C
90.0 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Eurostar Starglas FF004 HDPE, Glass Fiber Filled
Starglas FF004 is a Glass Fiber Reinforced High Density Polyethylene ResinInformation provided by Eurostar.
CTE, linear, Transverse to Flow 162 µm/m-°C

@Temperature -30.0 - 100 °C
90.0 µin/in-°F

@Temperature -22.0 - 212 °F
ISO 11359-2
SABIC Innovative Plastics SABIC PPCOMPOUND 5310 PP
SABIC® PPcompound 5310 is a mineral filled, impact modified polypropylene TPO. This material combines scratch resistance and heat stability with exterior automotive weathering stability. The IMDS I..
CTE, linear, Transverse to Flow 162 µm/m-°C

@Temperature 23.0 - 60.0 °C
90.0 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP Thermocomp FF004 PE (Europe-Africa-Middle East)
LNP* THERMOCOMP* FF004 is a compound based on Polyethylene resin containing Glass Fiber.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.