Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 187 µm/m-°C

@Temperature -30.0 - 120 °C
104 µin/in-°F

@Temperature -22.0 - 248 °F
ISO 11359
Nyco NYLITE® Wollastonite in Polypropylene
Data for polypropylene reinforced with 15% Nyco NYLITE® Wollastonite. Polypropylene used is Braskem TI6200Q High Impact Copolymer 20 MFR -NBWollastonite (calcium metasilicate, or CaSiO3) is a natur..
CTE, linear, Transverse to Flow 188 µm/m-°C

@Temperature -30.0 - 30.0 °C
104 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP LUBRICOMP YL003 Polyester Elastomer
LNP* LUBRICOMP* YL003 is a compoudn based on Polyester Elastomer resin containing 15% PTFE. Added feature of this grade is: Wear Resistant.
CTE, linear, Transverse to Flow 188 µm/m-°C

@Temperature 23.0 - 60.0 °C
104 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP YF006A Polyester Elastomer (Europe-Africa-Middle East)
LNP* THERMOCOMP* YF006A is a compound based on Polyester Elastomer containing Glass Fiber.