Material Notes:
LNP* LUBRICOMP* YL003 is a compoudn based on Polyester Elastomer resin containing 15% PTFE. Added feature of this grade is: Wear Resistant.
Physical Properties Metric English Comments
Specific Gravity 1.28 g/cc
1.28 g/cc
ASTM D792
Density 1.27 g/cc
0.0459 lb/in³
ASTM D792
Moisture Absorption 0.330 %
0.330 %
50% RH, 24 hrs; ASTM D570
0.470 %
0.470 %
23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow >= 0.020 cm/cm

@Time 86400 sec
>= 0.020 in/in

@Time 24.0 hour
ASTM D955
Linear Mold Shrinkage, Transverse 0.010 - 0.030 cm/cm

@Time 86400 sec
0.010 - 0.030 in/in

@Time 24.0 hour
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 14.0 MPa
2030 psi
5 mm/min; ISO 527
43.0 MPa
6240 psi
Type I, 5 mm/min; ASTM D638
Elongation at Yield 14.2 %
14.2 %
Type I, 5 mm/min; ASTM D638
43.5 %
43.5 %
5 mm/min; ISO 527
Tensile Modulus 0.230 GPa
33.4 ksi
50 mm/min; ASTM D638
0.240 GPa
34.8 ksi
1 mm/min; ISO 527
Flexural Modulus 0.220 GPa
31.9 ksi
2 mm/min; ISO 178
0.230 GPa
33.4 ksi
1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 3.12 J/cm
5.85 ft-lb/in
ASTM D256
Izod Impact, Unnotched 4.55 J/cm
8.52 ft-lb/in
ASTM D4812
Izod Impact, Notched (ISO) 35.0 kJ/m²
16.7 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 42.0 kJ/m²
20.0 ft-lb/in²
80*10*4; ISO 180/1U
Dart Drop, Total Energy 25.0 J

@Temperature 23.0 °C
18.4 ft-lb

@Temperature 73.4 °F
ASTM D3763
Impact Test 24.0 J
17.7 ft-lb
Multiaxial Impact; ISO 6603
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 172 µm/m-°C

@Temperature -30.0 - 30.0 °C
95.6 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
CTE, linear, Transverse to Flow 188 µm/m-°C

@Temperature -30.0 - 30.0 °C
104 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696