Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 86.1 °C @Thickness 3.18 mm |
187 °F @Thickness 0.125 in |
Annealed; ASTM D648 |
PolyOne Geon™ HTX Ultra LA426 Tan 3725 Polyvinyl Chloride Alloy (PVC Alloy) Optimum for Black and Darker Colors between 50 and 70 L value. Also suitable for colors above 70 L value.Recommend drying material for a minimum of 2 hours at 160 degrees Farenheit. Physical propert.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 86.1 °C @Thickness 3.18 mm |
187 °F @Thickness 0.125 in |
Annealed; ASTM D648 |
PolyOne Geon™ HTX Ultra LA426G Black 2880 Polyvinyl Chloride Alloy (PVC Alloy) Higher gloss version of Geon HTX Ultra LA426Recommend drying material for a minimum of 2 hours at 160 degrees Farenheit. Physical properties measured on LA426G Black 2880.Information provided by Pol.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 86.1 °C @Thickness 3.18 mm |
187 °F @Thickness 0.125 in |
Unannealed; ASTM D648 |
PolyOne Geon™ HTX Ultra LA427Plus Polyvinyl Chloride Alloy (PVC Alloy) Recommend drying material for a minimum of 2 hours at 160 degrees Farenheit. Physical properties based on Geon HTX Ultra LA427Plus Natural 0000Information provided by PolyOne |