Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 96.0 °C

@Thickness 12.7 mm
205 °F

@Thickness 0.500 in
Unannealed; ASTM-D648
Ineos ABS Lustran® 633 ABS, Injection Molding Grade
Lustran® ABS 633 is a general-purpose injection molding grade of ABS (Acrylonitrile Butadiene Styrene). It offers a good balance of physical properties, high gloss, and good moldability. Typical ..