Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 96.0 °C

@Thickness 12.7 mm
205 °F

@Thickness 0.500 in
Unannealed; ASTM-D648
Ineos ABS Lustran® 633 ABS, Injection Molding Grade
Lustran® ABS 633 is a general-purpose injection molding grade of ABS (Acrylonitrile Butadiene Styrene). It offers a good balance of physical properties, high gloss, and good moldability. Typical ..
Deflection Temperature at 0.46 MPa (66 psi) 96.1 °C

@Thickness 6.35 mm
205 °F

@Thickness 0.250 in
Unannealed; ASTM-D648
Ineos ABS Triax® 3050 ABS/Nylon Alloy, Injection Molding Grade (Conditioned)
Triax® 3050 resin is an ABS (Acrylonitrile Butadiene Styrene)/Nylon 6 alloy for injection molding. It is a semicrystalline thermoplastic with improved stability to light exposure, excellent proce..
Deflection Temperature at 0.46 MPa (66 psi) 96.1 °C

@Thickness 3.20 mm
205 °F

@Thickness 0.126 in
Unannealed; ASTM D648
Styron Magnum™ 1150 EM Acrylonitrile Butadiene Styrene (ABS)
Overview: MAGNUM™ ABS resins are thermoplastic materials which provide an excellent balance to processability, impact resistance and heat resistance as imparted by the various polymer compositions...