Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 81.1 °C @Thickness 6.35 mm |
178 °F @Thickness 0.250 in |
Annealed; ASTM D648 |
PolyOne Geon™ HTX M6307 Polyvinyl Chloride Alloy (PVC Alloy) Information provided by PolyOne |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 81.1 °C @Thickness 3.18 mm |
178 °F @Thickness 0.125 in |
Annealed; ASTM D648 |
PolyOne Geon™ Vinyl Dry Blend E7000 Polyvinyl Chloride, Rigid (PVC, Rigid) 60 degree gloss comparisons: Geon E7000 is 47-49;Geon E7456 is 40-49;Geon E7130 is 38-43;Geon E7370 is 26-31Information provided by PolyOne |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 81.1 °C @Thickness 3.18 mm |
178 °F @Thickness 0.125 in |
Annealed; ASTM D648 |
PolyOne Geon™ Vinyl Dry Blend E7001 Polyvinyl Chloride, Rigid (PVC, Rigid) 60 degree gloss comparisons: Geon E7001 is 27-29; Geon E7456 is 40-49; Geon E7130 is 38-43; Geon E7370 is 26-31Information provided by PolyOne |