Deflection Temperature at 0.46 MPa (66 psi) | 81.1 °C @Thickness 6.35 mm |
178 °F @Thickness 0.250 in |
Annealed; ASTM D648 |
PolyOne Geon™ HTX M6307 Polyvinyl Chloride Alloy (PVC Alloy) Information provided by PolyOne |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 81.1 °C @Thickness 3.18 mm |
178 °F @Thickness 0.125 in |
Annealed; ASTM D648 |
PolyOne Geon™ Vinyl Dry Blend E7000 Polyvinyl Chloride, Rigid (PVC, Rigid) 60 degree gloss comparisons: Geon E7000 is 47-49;Geon E7456 is 40-49;Geon E7130 is 38-43;Geon E7370 is 26-31Information provided by PolyOne |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 81.1 °C @Thickness 3.18 mm |
178 °F @Thickness 0.125 in |
Annealed; ASTM D648 |
PolyOne Geon™ Vinyl Dry Blend E7001 Polyvinyl Chloride, Rigid (PVC, Rigid) 60 degree gloss comparisons: Geon E7001 is 27-29; Geon E7456 is 40-49; Geon E7130 is 38-43; Geon E7370 is 26-31Information provided by PolyOne |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 81.0 °C @Thickness 3.20 mm |
178 °F @Thickness 0.126 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics Noryl N750T PPE+HIPS ECO-FLO(tm). ECO conforming, nonhalogenated flame retardant PPE+PS. High flow. Electrical, TV and Business equipment applications.This data was supplied by SABIC-IP for the Americas region. |