Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 99.0 °C | 210 °F | TM R050-25 |
Resinlab® SEC1244 Silver Filled Epoxy Adhesive Resinlab™ SEC1244 is a silver filled, two component, elevated temperature curing epoxy adhesive. It provides excellent electrical conductivity useful in many electronic applications. It is a smooth.. |
|||
Glass Transition Temp, Tg | 99.0 °C | 210 °F | |
Eastman Tenite 131E-28 Cellulose Acetate
(discontinued **) 28% plasticized and contains 50% fiber grade ester.ISO data as provided by the manufacturer, Eastman Chemical. |
|||
Glass Transition Temp, Tg | 99.0 °C | 210 °F | |
Lucite International Elvacite ® 3009 Acrylic Resin Elvacite® 3009 is a medium to high viscosity, methyl methacrylate based bead resin specially designed for use in plastic and vinyl coatings and inks.Information provided by Lucite International |
|||
Glass Transition Temp, Tg | 99.0 °C | 210 °F | |
Lucite International Elvacite ® 4062 Acrylic Resin Elvacite® 4062 is a solid bead resin specially designed for use in coatings for plastics, such as ABS, PS and PVC. It has good compatibility with many binders and plasticisers, and has excellent .. |
|||
Glass Transition Temp, Tg | 99.0 °C | 210 °F | Ultimate Tg |
Tra-Con Tra-Bond 342-13ACC Single Component Low Viscosity Epoxy Adhesive TRA-BOND 342-13ACC single component, low viscosity epoxy adhesive exhibits high bond strength and excellent thermal shock characteristics. This adhesive may be cured at room temperature in 24 hours .. |
|||
Glass Transition Temp, Tg | 99.0 °C | 210 °F | 90 Minute UV Cure + Thermal; DMA, E" |
3D Systems Accura® SI 40 Plastic for the SLA® 250 System Accura 40 "Ar" or "Hc" type materials - for the SLA 250 system. Mimics Nylon 6:6ApplicationsHigh temperature testing:Under hood bolt-on testingWind tunnel testingHVAC testingPrototyping and testing .. |
|||
Glass Transition Temp, Tg | 99.0 °C | 210 °F | wet |
Henkel Hysol EA 9628 Film Adhesive First generation, modified epoxy film, good stress, environmental resistance and structural propertiesApplications: Composite Bonding, Metal & Honeycomb BondingData from .060 psf, 300 g/m2 |