Polymer Property : Glass Transition Temp, Tg = 210 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 99.0 °C
210 °F
TM R050-25
Resinlab® SEC1244 Silver Filled Epoxy Adhesive
Resinlab™ SEC1244 is a silver filled, two component, elevated temperature curing epoxy adhesive. It provides excellent electrical conductivity useful in many electronic applications. It is a smooth..
Glass Transition Temp, Tg 99.0 °C
210 °F
Eastman Tenite 131E-28 Cellulose Acetate  (discontinued **)
28% plasticized and contains 50% fiber grade ester.ISO data as provided by the manufacturer, Eastman Chemical.
Glass Transition Temp, Tg 99.0 °C
210 °F
Lucite International Elvacite ® 3009 Acrylic Resin
Elvacite® 3009 is a medium to high viscosity, methyl methacrylate based bead resin specially designed for use in plastic and vinyl coatings and inks.Information provided by Lucite International
Glass Transition Temp, Tg 99.0 °C
210 °F
Lucite International Elvacite ® 4062 Acrylic Resin
Elvacite® 4062 is a solid bead resin specially designed for use in coatings for plastics, such as ABS, PS and PVC. It has good compatibility with many binders and plasticisers, and has excellent ..
Glass Transition Temp, Tg 99.0 °C
210 °F
Ultimate Tg
Tra-Con Tra-Bond 342-13ACC Single Component Low Viscosity Epoxy Adhesive
TRA-BOND 342-13ACC single component, low viscosity epoxy adhesive exhibits high bond strength and excellent thermal shock characteristics. This adhesive may be cured at room temperature in 24 hours ..
Glass Transition Temp, Tg 99.0 °C
210 °F
90 Minute UV Cure + Thermal; DMA, E"
3D Systems Accura® SI 40 Plastic for the SLA® 250 System
Accura 40 "Ar" or "Hc" type materials - for the SLA 250 system. Mimics Nylon 6:6ApplicationsHigh temperature testing:Under hood bolt-on testingWind tunnel testingHVAC testingPrototyping and testing ..
Glass Transition Temp, Tg 99.0 °C
210 °F
wet
Henkel Hysol EA 9628 Film Adhesive
First generation, modified epoxy film, good stress, environmental resistance and structural propertiesApplications: Composite Bonding, Metal & Honeycomb BondingData from .060 psf, 300 g/m2