Polymer Property : Glass Transition Temp, Tg = 106 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 41.0 °C
106 °F
ASTM E1545-00
DSM Somos® WaterClear® 10110 Epoxy Resin for Stereolithography  (discontinued **)
DescriptionDSM Somos® 10110 is a high-speed liquid photopolymer that produces strong, rigid, and durable parts with optical clarity using stereolithography machines. This material is especially us..
Glass Transition Temp, Tg 41.0 °C
106 °F
Lucite International Elvacite ® 2014 Acrylic Resin
Elvacite® 2014 is a medium molecular weight methyl methacrylate copolymer. 2014 is the softest and most flexible of the Elvacite® copolymer grades. It provides good pigment wetting. ElvaciteÂ..
Glass Transition Temp, Tg 41.0 °C
106 °F
Styron DL 242NA Functionalized SB
Performance Features: Glass fiber sizing, reactive with external cross-linkersApplications: Fiber Binding, Glass Fiber Binding, Nonwovens and Thermo MoldableLatin America/South AmericaInformation pr..
Glass Transition Temp, Tg 41.0 - 43.0 °C
106 - 109 °F
ASTM E1545-00
DSM Somos® GP Plus 14122
Somos® GP Plus 14122 is a low-viscosity stereolithography resin with an opaque white appearance. This material mirrors production plastics like ABS and PBT, making it an ideal choice for virtually ..
Glass Transition Temp, Tg 41.0 °C
106 °F
dynamic; DIN 53 736
Hippe PA 12 Nylon 12
Maintenance-free bearing and gear components under water, insulated components, seals, gear wheels. Parts for pumps and household units. Application in the electrical sector - less water absorptio..
Glass Transition Temp, Tg 41.0 °C
106 °F
3M Scotch-Weld™ DP605NS Structural Adhesive
3M™ Scotch-Weld™ Urethane Adhesives are two-part, non-sag urethane adhesives. They feature tough, flexible bonds with good adhesion to a wide variety of substrates especially wood and many properl..