Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Hippe PA 12 Nylon 12

Category Polymer , Thermoplastic , Nylon , Nylon 12
Manufacturer Erhard Hippe KG
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hippe PA 12 Nylon 12.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Maintenance-free bearing and gear components under water, insulated components, seals, gear wheels. Parts for pumps and household units. Application in the electrical sector - less water absorption than with PA 11.Information provided by Hippe.
Physical Properties Metric English Comments
Specific Gravity 1.02 g/cc
1.02 g/cc
DIN 53 479
Moisture Absorption at Equilibrium 0.70 %
0.70 %
Absorption of humidity in standard operating environment; DIN 53 715
Water Absorption at Saturation 1.6 %
1.6 %
DIN 53 495
Mechanical Properties Metric English Comments
Ball Indentation Hardness 95.0 MPa

@Time 30.0 sec
13800 psi

@Time 0.00833 hour
DIN 53 456
Tensile Strength 35.0 MPa
5080 psi
DIN 53 455
Elongation at Break 240 %
240 %
DIN 53 455
Tensile Modulus 1.80 GPa
261 ksi
DIN 53 457
Charpy Impact, Notched NB
NB
DIN 53 453
Coefficient of Friction, Dynamic 0.32 - 0.38
0.32 - 0.38
Against steel, p=0.05 N/mm², v=0.6 m/s, hardened and ground
Tear Strength Test 46 - 52
46 - 52
in MPa; DIN 53 455
Abrasion 0.80
0.80
µm/km; Against steel, p=0.05 N/mm², v=0.6 m/s, hardened and ground
Thermal Properties Metric English Comments
CTE, linear 100 µm/m-°C
55.6 µin/in-°F
Specific Heat Capacity 2.10 J/g-°C
0.502 BTU/lb-°F
Thermal Conductivity 0.230 W/m-K
1.60 BTU-in/hr-ft²-°F
Melting Point 179 °C
354 °F
DIN 53 736
Maximum Service Temperature, Air 80.0 °C
176 °F
Continuous use
150 °C
302 °F
Short Periods
Deflection Temperature at 0.46 MPa (66 psi) 140 °C
284 °F
ISO-R 75 Method B
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °C
122 °F
ISO-R 75 Method A
Glass Transition Temp, Tg 41.0 °C
106 °F
dynamic; DIN 53 736
Flammability, UL94 V-2
V-2
Electrical Properties Metric English Comments
Volume Resistivity 2.00e+15 ohm-cm
2.00e+15 ohm-cm
DIN 53 482, VDE 0303, Part 3
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
DIN 53 482
Dielectric Constant 3.6

@Frequency 1.00e+6 Hz
3.6

@Frequency 1.00e+6 Hz
DIN 53 483, IEC-250
Dielectric Strength 33.0 kV/mm
838 kV/in
Breakdown; DIN 53 481, IEC-243, VDE 0303 Part 1
Dielectric Loss Index 0.040

@Frequency 1.00e+6 Hz
0.040

@Frequency 1.00e+6 Hz
DIN 53 483, IEC-250
Descriptive Properties Value Comments
Color natural
Creep Resistance Grade CTI 600
DIN 53 480, IEC-112, VDE 0303 Part 1
Resistance to hot water, suds resistant
Users viewing this material also viewed the following: