Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 2.09 J/g-°C | 0.500 BTU/lb-°F | 8HS form; ASTM C351 |
Park Electrochemical Nelcote® F-555 Phenolic Prepreg, ENKA Reinforced Nelcote® F-555 is a carbon-filled MIL-R-9299 phenolic resin optimized for coating Carbonized Rayon cloth. F-555 is used extensively in the manufacture of high temperature rocket nozzles, heat shiel.. |
|||
Specific Heat Capacity | 2.09 J/g-°C | 0.500 BTU/lb-°F | |
Trelleborg AEM Syntac® 350 Syntactic Foam Syntac® 350 is made from high grade epoxy resin and hollow glass microspheres designed specifically for fabricating thermoforming plugs and other associated tooling.Available in block, sheet and ro.. |
|||
Specific Heat Capacity | 2.09 J/g-°C | 0.500 BTU/lb-°F | |
Trelleborg AEM Syntac® 351 Syntactic Foam Syntac® 351 is a castable syntactic composite material of epoxy resin and high performance hollow glass microspheres designed specifically for molding thermoforming plugs and other associated tooli.. |
|||
Specific Heat Capacity | 2.09 J/g-°C | 0.500 BTU/lb-°F | |
Trelleborg Emerson & Cuming Syntac® 350 Composite Materials Syntactic Foam Syntac 350 foam is a rigid, high strength composite of epoxy resin and microscopic hollow glass microspheres designed specifically for fabricating thermoforming plugs and other associated tooling. .. |
|||
Specific Heat Capacity | 2.09 J/g-°C | 0.500 BTU/lb-°F | |
DuPont Performance Polymers Crastin® FG6129 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)< Unreinforced High Viscosity Polybutylene Terephthalate Developed for Food Contact Applications and Extrusion and Injection Molding Crastin FG6129 NC010 is an unreinforced high viscosity polybutylene.. |
|||
Specific Heat Capacity | 2.09 J/g-°C @Temperature 20.0 °C |
0.500 BTU/lb-°F @Temperature 68.0 °F |
|
Dow VORANOL™ 4240 Polyether Polyol VORANOL™ 4240 polyether polyol is a nominal 4000 molecular weight diol based on propylene oxide with ethylene oxide capping. Its high molecular weight and enhanced reactivity make it well suited t.. |
|||
Specific Heat Capacity | 2.09 J/g-°C | 0.500 BTU/lb-°F | |
Trelleborg AEM Syntac® 450 Syntactic Foam Syntac® 450 syntactic foam is the high temperature (450°F/232°C) member of the Syntac® product family.A rigid, high strength composite of epoxy resin and hollow glass microspheres, Syntac® 450 .. |
|||
Specific Heat Capacity | 2.09 J/g-°C @Thickness 1.50 mm |
0.500 BTU/lb-°F @Thickness 0.0591 in |
|
DuPont Performance Polymers Zytel® 70G25HSLR NC010 Nylon 66
(Unverified Data**) 25% Glass Reinforced Heat Stabilized Hydrolysis Resistant Polyamide 66 Zytel 70G25HSLR NC010 is a 25% glass fiber reinforced heat stabilized hydrolysis resistant polyamide 66 resin for injection mol.. |