Specific Heat Capacity 2.09 J/g-°C
0.500 BTU/lb-°F
8HS form; ASTM C351
Park Electrochemical Nelcote® F-555 Phenolic Prepreg, ENKA Reinforced
Nelcote® F-555 is a carbon-filled MIL-R-9299 phenolic resin optimized for coating Carbonized Rayon cloth. F-555 is used extensively in the manufacture of high temperature rocket nozzles, heat shiel..
Specific Heat Capacity 2.09 J/g-°C
0.500 BTU/lb-°F
Trelleborg AEM Syntac® 350 Syntactic Foam
Syntac® 350 is made from high grade epoxy resin and hollow glass microspheres designed specifically for fabricating thermoforming plugs and other associated tooling.Available in block, sheet and ro..
Specific Heat Capacity 2.09 J/g-°C
0.500 BTU/lb-°F
Trelleborg AEM Syntac® 351 Syntactic Foam
Syntac® 351 is a castable syntactic composite material of epoxy resin and high performance hollow glass microspheres designed specifically for molding thermoforming plugs and other associated tooli..
Specific Heat Capacity 2.09 J/g-°C
0.500 BTU/lb-°F
Trelleborg Emerson & Cuming Syntac® 350 Composite Materials Syntactic Foam
Syntac 350 foam is a rigid, high strength composite of epoxy resin and microscopic hollow glass microspheres designed specifically for fabricating thermoforming plugs and other associated tooling. ..
Specific Heat Capacity 2.09 J/g-°C
0.500 BTU/lb-°F
DuPont Performance Polymers Crastin® FG6129 NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)<
Unreinforced High Viscosity Polybutylene Terephthalate Developed for Food Contact Applications and Extrusion and Injection Molding Crastin FG6129 NC010 is an unreinforced high viscosity polybutylene..
Specific Heat Capacity 2.09 J/g-°C

@Temperature 20.0 °C
0.500 BTU/lb-°F

@Temperature 68.0 °F
Dow VORANOL™ 4240 Polyether Polyol
VORANOL™ 4240 polyether polyol is a nominal 4000 molecular weight diol based on propylene oxide with ethylene oxide capping. Its high molecular weight and enhanced reactivity make it well suited t..
Specific Heat Capacity 2.09 J/g-°C
0.500 BTU/lb-°F
Trelleborg AEM Syntac® 450 Syntactic Foam
Syntac® 450 syntactic foam is the high temperature (450°F/232°C) member of the Syntac® product family.A rigid, high strength composite of epoxy resin and hollow glass microspheres, Syntac® 450 ..
Specific Heat Capacity 2.09 J/g-°C

@Thickness 1.50 mm
0.500 BTU/lb-°F

@Thickness 0.0591 in
DuPont Performance Polymers Zytel® 70G25HSLR NC010 Nylon 66  (Unverified Data**)
25% Glass Reinforced Heat Stabilized Hydrolysis Resistant Polyamide 66 Zytel 70G25HSLR NC010 is a 25% glass fiber reinforced heat stabilized hydrolysis resistant polyamide 66 resin for injection mol..