Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.530 J/g-°C @Temperature 100 °C |
0.127 BTU/lb-°F @Temperature 212 °F |
|
Outokumpu 2205 Duplex Stainless Steel Duplex stainless combining high mechanical strength with good corrosion resistance.Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical t.. |
|||
Specific Heat Capacity | 0.530 J/g-°C @Temperature 500 °C |
0.127 BTU/lb-°F @Temperature 932 °F |
|
Outokumpu 4828 High Temperature Austenitic Stainless Steel Standardized high temperature steel for service at temperatures of up to 950-1000°C in dry air. Utilization in the temperature range of 600-900°C can lead to embrittlement.Applications: Heat and .. |
|||
Specific Heat Capacity | 0.530 J/g-°C @Temperature 500 °C |
0.127 BTU/lb-°F @Temperature 932 °F |
|
Outokumpu 4833 High Temperature Austenitic Stainless Steel Standardized high temperature steel for service at temperatures of up to 950-1000°C in dry air. Utilization in the temperature range of 600-900°C can lead to embrittlement.Applications: Heat and .. |
|||
Specific Heat Capacity | 0.530 J/g-°C @Temperature 500 °C |
0.127 BTU/lb-°F @Temperature 932 °F |
|
Outokumpu 4841 High Temperature Austenitic Stainless Steel Variant of 1.4845 with an increased silicon content which enhances the steel's resistance to oxidation/corrosion but has also made it more susceptible to embrittlement.Applications: Heat and creep r.. |
|||
Specific Heat Capacity | 0.530 J/g-°C @Temperature 500 °C |
0.127 BTU/lb-°F @Temperature 932 °F |
|
Outokumpu 4845 High Temperature Austenitic Stainless Steel Standardized high-temperature steel for use at temperatures up to 1100°C in dry air. Prone to embrittlement after exposure between 600-900°C. Applications: Heat and creep resistance. For use o.. |
|||
Specific Heat Capacity | 0.530 J/g-°C @Temperature 500 °C |
0.127 BTU/lb-°F @Temperature 932 °F |
|
Outokumpu 4878 High Temperature Austenitic Stainless Steel Heat-resistant variant of 1.4541, with a slightly higher max carbon content. Recommended max service temperature for this steel in dry air is 800°C. Applications: Heat and creep resistance. For .. |
|||
Specific Heat Capacity | 0.530 J/g-°C @Temperature 100 °C |
0.127 BTU/lb-°F @Temperature 212 °F |
|
Outokumpu SAF 2304® Duplex Stainless Steel Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical tankersSeawater systemsFirewalls and blast walls on offshore platformsBridgesCompone.. |
|||
Specific Heat Capacity | 0.530 J/g-°C @Temperature 100 °C |
0.127 BTU/lb-°F @Temperature 212 °F |
|
Outokumpu SAF 2507® Duplex Stainless Steel Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical tankersSeawater systemsFirewalls and blast walls on offshore platformsBridgesCompone.. |
|||
Specific Heat Capacity | 0.530 J/g-°C | 0.127 BTU/lb-°F | |
Schott N-LASF44 Glass Information Provided by SCHOTT North America, Inc. |
|||
Specific Heat Capacity | 0.530 J/g-°C | 0.127 BTU/lb-°F | |
Schott N-LASF9 Glass Information Provided by SCHOTT North America, Inc. |
|||
Specific Heat Capacity | 0.530 J/g-°C | 0.127 BTU/lb-°F | |
Schott P-SF67 Glass Suitable for precision moldingInformation Provided by SCHOTT North America, Inc. |
|||
Specific Heat Capacity | 0.530 J/g-°C @Temperature 500 °C |
0.127 BTU/lb-°F @Temperature 932 °F |
|
Outokumpu 4948 High Temperature Austenitic Stainless Steel Creep-resistant variant of 1.4301, with a standardized minimum carbon content for service at temperatures of up to 800°C in dry air.Applications: Heat and creep resistance. For use over 550°C for.. |
|||
Specific Heat Capacity | 0.530 J/g-°C @Temperature 100 °C |
0.127 BTU/lb-°F @Temperature 212 °F |
|
Outokumpu LDX 2101® Duplex Stainless Steel Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical tankersSeawater systemsFirewalls and blast walls on offshore platformsBridgesCompone.. |