Thermal Properties Metric English Comments
Specific Heat Capacity 1.67 J/g-°C
0.400 BTU/lb-°F
Ensinger Tecamid® 6/6 Nylon (PA66)
Type 6/6 is a general purpose standard grade nylon. Extruded in natural and black. (Weather Resistant Black Grade is also available.)Information provided by Ensinger, Inc.
Specific Heat Capacity 1.67 J/g-°C
0.400 BTU/lb-°F
Ensinger Tecamid® MDS® Molybdenum Disulfide Filled Nylon (PA)
Tecamid MDS® has enhanced surface lubricity and wear resistance over unfilled nylon. It is an ideal material to replace metals in machinery. Low surface friction Increased surface hardness Incre..
Specific Heat Capacity 1.67 J/g-°C
0.400 BTU/lb-°F
Ensinger Tecast™ 6PA Natural Unfilled Cast Nylon 6 (PA6)
Tecast® 6PA Natural is an FDA-compliant grade used in applications requiring cast nylon but without any fillers.General Tecast® Cast Nylon Information: Tecast cast nylon, available in a variety of..
Specific Heat Capacity 1.67 J/g-°C
0.400 BTU/lb-°F
Ensinger Tecast Vekton™ 6PA Black Unfilled Cast Nylon 6 (PA6)
Tecast® 6PA Black is a black cast nylon that is more UV resistant than natural nylon 6.General Tecast® Cast Nylon Information: Tecast cast nylon, available in a variety of grades, offers a combina..
Specific Heat Capacity 1.67 J/g-°C
0.400 BTU/lb-°F
Ensinger Tecast Vekton™ 6PA Blue Unfilled Cast Nylon 6 (PA6)
Tecast 6PA Blue is a blue cast nylon with properties similar to natural nylon 6.General Tecast Cast Nylon Information: Tecast cast nylon, available in a variety of grades, offers a combination of go..