Thermal Properties Metric English Comments
Specific Heat Capacity 1.47 J/g-°C
0.351 BTU/lb-°F
IEC 1006
Polycasa XT PMMA
QUINN XT sheets have good optical properties and a brilliant surface. QUINN XT sheets offer excellent transparency, good mechanical properties, are UV resistant, have very good weathering and ageing..
Specific Heat Capacity 1.47 J/g-°C
0.351 BTU/lb-°F
ASTM C351
Lucite International XL Sanitary Ware Acrylic Sheet
Lucite® XL continuous-cast cross-linked acrylic sheet is specially formulated for deep-draw thermoforming. It is used primarily for production of spas.Benefits: Smooth surface; Infinite colors an..
Specific Heat Capacity 1.47 J/g-°C
0.351 BTU/lb-°F
Hippe PMMA
Components made of PMMA are brilliantly transparent. Outstanding aging stability and weathering resistance. Good surface hardness. Abrasion-resistant. Physiologically safe. High strength. Easi..
Specific Heat Capacity 1.47 J/g-°C
0.351 BTU/lb-°F
Average value: 1.47 J/g-°C Grade Count:8
Overview of materials for Acrylic, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Extruded". Each property range of values reported is minimum and maximum values of appropriate ..
Specific Heat Capacity 1.47 J/g-°C
0.351 BTU/lb-°F
Average value: 1.47 J/g-°C Grade Count:6
Overview of materials for Acrylic, Cast
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Cast". Each property range of values reported is minimum and maximum values of appropriate MatW..
Specific Heat Capacity 1.47 J/g-°C
0.351 BTU/lb-°F
ASTM C177
Kleerdex Elson® 405 AS DC Plate, PMMA/Acrylic, Clear Transparent  (discontinued **)
Information provided by Kleerdex Company. Kleerdex Company became KYDEX, LLC in 2009.