Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 1.47 J/g-°C | 0.351 BTU/lb-°F | IEC 1006 |
Polycasa XT PMMA QUINN XT sheets have good optical properties and a brilliant surface. QUINN XT sheets offer excellent transparency, good mechanical properties, are UV resistant, have very good weathering and ageing.. |
|||
Specific Heat Capacity | 1.47 J/g-°C | 0.351 BTU/lb-°F | ASTM C351 |
Lucite International XL Sanitary Ware Acrylic Sheet Lucite® XL continuous-cast cross-linked acrylic sheet is specially formulated for deep-draw thermoforming. It is used primarily for production of spas.Benefits: Smooth surface; Infinite colors an.. |
|||
Specific Heat Capacity | 1.47 J/g-°C | 0.351 BTU/lb-°F | |
Hippe PMMA Components made of PMMA are brilliantly transparent. Outstanding aging stability and weathering resistance. Good surface hardness. Abrasion-resistant. Physiologically safe. High strength. Easi.. |
|||
Specific Heat Capacity | 1.47 J/g-°C | 0.351 BTU/lb-°F | Average value: 1.47 J/g-°C Grade Count:8 |
Overview of materials for Acrylic, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Extruded". Each property range of values reported is minimum and maximum values of appropriate .. |
|||
Specific Heat Capacity | 1.47 J/g-°C | 0.351 BTU/lb-°F | Average value: 1.47 J/g-°C Grade Count:6 |
Overview of materials for Acrylic, Cast This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Cast". Each property range of values reported is minimum and maximum values of appropriate MatW.. |
|||
Specific Heat Capacity | 1.47 J/g-°C | 0.351 BTU/lb-°F | ASTM C177 |
Kleerdex Elson® 405 AS DC Plate, PMMA/Acrylic, Clear Transparent
(discontinued **) Information provided by Kleerdex Company. Kleerdex Company became KYDEX, LLC in 2009. |