Polymer Property : Specific Heat Capacity = 0.2093 J/g-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Specific Heat Capacity 0.2093 J/g-°C
0.05002 BTU/lb-°F
CoorsTek ACI-Co6 Tungsten Carbide
Applications: seal rings, plungers, liners, nozzles, valve components, pump components, wear components in the oil & gas, construction, and agriculture equipment industries