Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.2093 J/g-°C | 0.05002 BTU/lb-°F | |
CoorsTek ACI-Co6 Tungsten Carbide Applications: seal rings, plungers, liners, nozzles, valve components, pump components, wear components in the oil & gas, construction, and agriculture equipment industries |