Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.840 - 0.880 J/g-°C | 0.201 - 0.210 BTU/lb-°F | |
PEAK Werkstoff DISPAL S263 Aluminum Alloy, AlSi25Cu3Fe3Ni3MgCoTi, Condition T6 Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational.. |
|||
Specific Heat Capacity | 0.840 - 0.880 J/g-°C | 0.201 - 0.210 BTU/lb-°F | |
PEAK Werkstoff DISPAL S263 Aluminum Alloy, AlSi25Cu3Fe3Ni3MgCoTi, Condition F Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational.. |
|||
Specific Heat Capacity | 0.840 - 0.880 J/g-°C | 0.201 - 0.210 BTU/lb-°F | |
PEAK Werkstoff DISPAL S263 Aluminum Alloy, AlSi25Cu3Fe3Ni3MgCoTi, Condition T4 Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational.. |
|||
Specific Heat Capacity | 0.840 J/g-°C | 0.201 BTU/lb-°F | |
Microtherm Group MT Thermosphere® Moldable Insulation Paste MT Thermosphere® is a low density temperature resistant paste with excellent thermal insulation properties from cryogenic to high temperature exposure. It is a perfectly seamless insulation syste.. |
|||
Specific Heat Capacity | 0.840 J/g-°C | 0.201 BTU/lb-°F | |
Schott N-BAF51 Glass Information Provided by SCHOTT North America, Inc. |
|||
Specific Heat Capacity | 0.840 J/g-°C | 0.201 BTU/lb-°F | |
Skamol Group SUPER 1100 E Calcium Silicate Insulating Slab SKAMOL SUPER calcium silicate slabs have the following characteristics: Max. service temperature: Up to 1100°C (2012°F)Back-up insulation onlyExtremely lightweightVery low thermal conductivity.. |
|||
Specific Heat Capacity | 0.840 J/g-°C | 0.201 BTU/lb-°F | |
Skamol Group SUPER 1100 ET Calcium Silicate Insulating Slab SKAMOL SUPER calcium silicate slabs have the following characteristics: Max. service temperature: Up to 1100°C (2012°F)Back-up insulation onlyExtremely lightweightVery low thermal conductivity.. |
|||
Specific Heat Capacity | 0.840 J/g-°C | 0.201 BTU/lb-°F | |
Skamol Group SUPER ISOL Calcium Silicate Insulating Slab SKAMOL SUPER calcium silicate slabs have the following characteristics: Max. service temperature: Up to 1100°C (2012°F)Back-up insulation onlyExtremely lightweightVery low thermal conductivity.. |
|||
Specific Heat Capacity | 0.840 J/g-°C | 0.201 BTU/lb-°F | DSC |
Wolf Kunststoff ZEDEX® ZX-530EL3 066 Polymer Alloy, Carbon Fiber Reinforced Main Characteristics: Low thermal expansion; High rigidity; High yield stress; High wear resistance; Low friction; Stress ResistantApplications: Chemical Engineering; Laboratory Technology; Automitv.. |
|||
Specific Heat Capacity | 0.841 J/g-°C | 0.201 BTU/lb-°F | through-plane |
Bulk Molding Compounds BMC 940 Vinyl Ester Bipolar Plate Material Bulk Molding Compounds, Inc. is the largest manufacturer of thermoset bulk molding compounds in North America, serving the automotive, appliance, and electrical markets. BMC thermosets are the most .. |
|||
Specific Heat Capacity | 0.841 - 1.51 J/g-°C | 0.201 - 0.360 BTU/lb-°F | Average value: 1.28 J/g-°C Grade Count:3 |
Overview of materials for Vinyl Ester Sheet Molding Compound This property data is a summary of similar materials in the MatWeb database for the category "Vinyl Ester Sheet Molding Compound". Each property range of values reported is minimum and maximum value.. |