Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.435 J/g-°C @Temperature 200 °C |
0.104 BTU/lb-°F @Temperature 392 °F |
|
Haynes 230® alloy, 10% cold reduction Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic.. |
|||
Specific Heat Capacity | 0.435 J/g-°C @Temperature 200 °C |
0.104 BTU/lb-°F @Temperature 392 °F |
|
Haynes 230® alloy, 20% cold reduction, 1066°C anneal for 5 minutes Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic.. |
|||
Specific Heat Capacity | 0.435 J/g-°C @Temperature 200 °C |
0.104 BTU/lb-°F @Temperature 392 °F |
|
Haynes 230® alloy, 20% cold reduction, 1177°C anneal for 5 minutes Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic.. |
|||
Specific Heat Capacity | 0.435 J/g-°C @Temperature 200 °C |
0.104 BTU/lb-°F @Temperature 392 °F |
|
Haynes 230® alloy, 30% cold reduction, 1177°C anneal for 5 minutes Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic.. |
|||
Specific Heat Capacity | 0.435 J/g-°C @Temperature 200 °C |
0.104 BTU/lb-°F @Temperature 392 °F |
|
Haynes 230® alloy, plate, 1000 hours exposure at 871°C (1600°F) Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic.. |
|||
Specific Heat Capacity | 0.435 J/g-°C @Temperature >=100 °C |
0.104 BTU/lb-°F @Temperature >=212 °F |
|
Haynes Multimet® alloy, 1.6 mm thick sheet, 1177°C heat treatment, rapid air cooled Recommended for use in applications involving high stress at temperatures up to 816°C (1500°F), and moderate stresses up to 1093°C (2000°F). Excellent oxidation resistance, good ductilit.. |
|||
Specific Heat Capacity | 0.435 J/g-°C @Temperature >=100 °C |
0.104 BTU/lb-°F @Temperature >=212 °F |
|
Haynes Multimet® alloy, 6.15 mm hot-rolled bar, 5% cold reduction Recommended for use in applications involving high stress at temperatures up to 816°C (1500°F), and moderate stresses up to 1093°C (2000°F). Excellent oxidation resistance, good ductilit.. |
|||
Specific Heat Capacity | 0.435 J/g-°C @Temperature >=100 °C |
0.104 BTU/lb-°F @Temperature >=212 °F |
|
Haynes Multimet® alloy, GTAW, 3.2 mm sheet Recommended for use in applications involving high stress at temperatures up to 816°C (1500°F), and moderate stresses up to 1093°C (2000°F). Excellent oxidation resistance, good ductilit.. |
|||
Specific Heat Capacity | 0.435 J/g-°C @Temperature >=100 °C |
0.104 BTU/lb-°F @Temperature >=212 °F |
|
Haynes Multimet® alloy, GTAW, 6.35 mm plate Recommended for use in applications involving high stress at temperatures up to 816°C (1500°F), and moderate stresses up to 1093°C (2000°F). Excellent oxidation resistance, good ductilit.. |
|||
Specific Heat Capacity | 0.435 J/g-°C @Temperature >=100 °C |
0.104 BTU/lb-°F @Temperature >=212 °F |
|
Haynes Multimet® alloy, sand cast, 1171°C heat treatment for 2 hours Recommended for use in applications involving high stress at temperatures up to 816°C (1500°F), and moderate stresses up to 1093°C (2000°F). Excellent oxidation resistance, good ductilit.. |
|||
Specific Heat Capacity | 0.435 J/g-°C @Temperature 200 °C |
0.104 BTU/lb-°F @Temperature 392 °F |
|
Haynes 230® alloy, plate, 8000 hours exposure at 871°C (1600°F) Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic.. |
|||
Specific Heat Capacity | 0.434 J/g-°C @Temperature 600 °C |
0.104 BTU/lb-°F @Temperature 1110 °F |
|
Haynes Hastelloy® B-3® alloy, 3.2 mm bright annealed sheet The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
Specific Heat Capacity | 0.436 J/g-°C @Temperature 500 °C |
0.104 BTU/lb-°F @Temperature 932 °F |
|
Haynes Hastelloy® B-3® alloy, 3.2 mm bright annealed sheet The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
Specific Heat Capacity | 0.436 J/g-°C @Temperature 500 °C |
0.104 BTU/lb-°F @Temperature 932 °F |
|
Haynes Hastelloy® B-3® alloy, 30% cold work The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
Specific Heat Capacity | 0.436 J/g-°C @Temperature 500 °C |
0.104 BTU/lb-°F @Temperature 932 °F |
|
Haynes Hastelloy® B-3® alloy, 40% cold work The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
Specific Heat Capacity | 0.434 J/g-°C @Temperature 600 °C |
0.104 BTU/lb-°F @Temperature 1110 °F |
|
Haynes Hastelloy® B-3® alloy, 50% cold work The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
Specific Heat Capacity | 0.435 J/g-°C | 0.104 BTU/lb-°F | |
HP Alloys Alloy 718, 20% Cold Worked 20% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Internati.. |
|||
Specific Heat Capacity | 0.435 J/g-°C | 0.104 BTU/lb-°F | |
HP Alloys Alloy 718, 25% Cold Worked, Aged 25% Cold Worked, Aged applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Int.. |
|||
Specific Heat Capacity | 0.435 J/g-°C | 0.104 BTU/lb-°F | |
HP Alloys Alloy 718, 30% Cold Worked, Aged 30% Cold Worked, Aged applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Int.. |
|||
Specific Heat Capacity | 0.435 J/g-°C @Temperature 20.0 - 100 °C |
0.104 BTU/lb-°F @Temperature 68.0 - 212 °F |
|
Special Metals DURANICKEL® 301 (UNS N03301) Annealed Rod and Bar Tensile strength (ultimate and yield), compressive strength, hardness, and elongation values reported here are typical for Annealed Rod and Bar specifically. Other property values are typical of ann.. |
|||
Specific Heat Capacity | 0.435 J/g-°C @Temperature 20.0 - 100 °C |
0.104 BTU/lb-°F @Temperature 68.0 - 212 °F |
|
Special Metals DURANICKEL® 301 (UNS N03301) Annealed Wire Tensile strength (ultimate) and elongation values reported here are typical for Annealed Wire specifically. Other property values are typical of annealed DURANICKEL® alloy 301 or the alloy in gen.. |
|||
Specific Heat Capacity | 0.435 J/g-°C | 0.104 BTU/lb-°F | |
Special Metals INCOLOY® Alloy 925 A precipitation-hardenable nickel-iron-chromium alloy with additions of molybdenum and copper. It combines the high strength of a precipitation-hardenable alloy with the excellent corrosion resista.. |
|||
Specific Heat Capacity | 0.436 J/g-°C | 0.104 BTU/lb-°F | |
Special Metals NIMONIC® Alloy PE11 A nickel-iron-chromium alloy precipitation hardened by titanium and aluminum and solid-solution strengthened by an addition of molybdenum. It was developed as a high-strength sheet alloy for use at.. |
|||
Specific Heat Capacity | 0.435 J/g-°C @Temperature 200 °C |
0.104 BTU/lb-°F @Temperature 392 °F |
|
Haynes 230® alloy, plate, 16000 hours exposure at 760°C (1400°F) Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applicat.. |
|||
Specific Heat Capacity | 0.435 J/g-°C @Temperature >=100 °C |
0.104 BTU/lb-°F @Temperature >=212 °F |
|
Haynes Multimet® alloy, 6.15 mm hot-rolled bar, 10% cold reduction Recommended for use in applications involving high stress at temperatures up to 816°C (1500°F), and moderate stresses up to 1093°C (2000°F). Excellent oxidation resistance, good ductility, and i.. |
|||
Specific Heat Capacity | 0.435 J/g-°C @Temperature >=100 °C |
0.104 BTU/lb-°F @Temperature >=212 °F |
|
Haynes Multimet® alloy, 6.15 mm hot-rolled bar, 25% cold reduction Recommended for use in applications involving high stress at temperatures up to 816°C (1500°F), and moderate stresses up to 1093°C (2000°F). Excellent oxidation resistance, good ductility, and i.. |
|||
Specific Heat Capacity | 0.435 J/g-°C | 0.104 BTU/lb-°F | |
HP Alloys Alloy 718, 5% Cold Worked 5% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Internatio.. |
|||
Specific Heat Capacity | 0.435 J/g-°C @Temperature 200 °C |
0.104 BTU/lb-°F @Temperature 392 °F |
|
Haynes 230® alloy, 50% cold reduction, 1177°C anneal for 5 minutes Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applicat.. |
|||
Specific Heat Capacity | 0.435 J/g-°C @Temperature 200 °C |
0.104 BTU/lb-°F @Temperature 392 °F |
|
Haynes 230® alloy, cold rolled and 1232°C solution annealed sheet Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applicat.. |
|||
Specific Heat Capacity | 0.435 J/g-°C @Temperature 200 °C |
0.104 BTU/lb-°F @Temperature 392 °F |
|
Haynes 230® alloy, plate, 4000 hours exposure at 871°C (1600°F) Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applicat.. |