Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | >= 982 °C | >= 1800 °F | approximate |
Schmolz + Bickenbach MoldMAX® V Copper Alloy Description: Brush Wellman’s MoldMAX® V (MMV) is a high conductivity, moderately high strength, copper nickel silicon chromium alloy. Applications include injection mold and blow mold cores .. |
|||
Melting Point | 982 °C | 1800 °F | |
Unifrax Fiberfrax® 440 Ceramic Fiber Paper 440 paper is a low-cost, high-strength composite paper made from a combination of ceramic fiber, inert fillers, and reinforcing fiberglass. The fiberglass gives added strength to the 440 paper at o.. |
|||
Melting Point | 982 - 1070 °C | 1800 - 1950 °F | |
Universal Wire Works BNi-4 (AMS 4779) Nickel Base Brazing Filler Metal Information provided by Universal Wire Works for their line of welding wire and filler metal. |