Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 949 - 1070 °C | 1740 - 1950 °F | |
Universal Wire Works BNi-1A (AMS 4776) Nickel Base Brazing Filler Metal Low Carbon (compare to BNi-1)Information provided by Universal Wire Works for their line of welding wire and filler metal. |
|||
Melting Point | 982 - 1070 °C | 1800 - 1950 °F | |
Universal Wire Works BNi-4 (AMS 4779) Nickel Base Brazing Filler Metal Information provided by Universal Wire Works for their line of welding wire and filler metal. |