Thermal Properties Metric English Comments
Melting Point 87.2 °C
189 °F
Peak Melting Temperature; ExxonMobil Method
ExxonMobil OPTEMA™ TC 115 Molding, extrusion and compounding resin  (discontinued **)
OPTEMA TC 115 is an ethylene methyl acrylate copolymer, which can be used as a compatibilizer and impact modifier for engineering thermoplastics. It has been processed at temperatures up to 625°F w..
Melting Point 87.2 °C
189 °F
Peak Melting Temperature; ExxonMobil Method
ExxonMobil ESCOR™ AT 310 Blown Film Resin  (discontinued **)
ESCOR AT 310 is an acid terpolymer which provides excellent adhesion to a variety of polar and non-polar materials such as metals, glass, polyolefins, polyamides, polyesters, etc. It is suitable fo..
Melting Point 87.2 °C
189 °F
Peak Melting Temperature; ExxonMobil Method
ExxonMobil ESCOR™ AT 310 Cast Film Resin  (discontinued **)
ESCOR AT 310 is an acid terpolymer which provides excellent adhesion to a variety of polar and non-polar materials such as metals, glass, polyolefins, polyamides, polyesters, etc. It is suitable fo..
Melting Point 87.2 °C
189 °F
Peak Melting Temperature; ExxonMobil Method
ExxonMobil Escorene® LD 725.21 Molding, extrusion, compounding and adhesive resin  (discontinued **)
Escorene Ultra LD 722.21 is 18 wt% vinyl acetate copolymer suitable for molding, extrusion, compounding and hot melt adhesive applications.Information provided by ExxonMobil Chemical
Melting Point 87.2 °C
189 °F
Peak Melting Temperature; ExxonMobil Method
ExxonMobil Escorene® LD 728.61 Molding, extrusion and compounding resin
Escorene Ultra LD 728.61 is a high vinyl acetate copolymer with low melting temperature and excellent strength properties and toughness.Availability: Latin America, North America and South America A..