Westlake EMAC® SP2409 20% EMA Copolymer

Category Polymer , Thermoplastic , Ethylene Methyl Acrylate
Manufacturer Westlake Chemical Corporation
Trade Name EMAC®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Westlake EMAC® SP2409 20% EMA Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Westlake EMAC� SP2409 is a 20% EMA copolymer designed for extrusion coating, tie-layers, and extrusions where flexibility, compatibility, low heat seal temperatures, or a high coefficient of friction are required. SP2409 provides excellent adhesion to polyolefins, polyesters, and other polymers while providing outstanding low temperature performance. Key attributes of SP2409 include: good heat & RF sealing, low temperature toughness, and a high coefficient of friction. It is soft, flexible, and tough without plasticizers. Its applications include: extrusion coating, flexible packaging, tie-layers, compatibilizer, heat seal layer, and high C.O.F. non-skid surfaces. This resin grade complies with 21 CFR 177.1340. EMAC� resins adhere to and are compatible with a wide range of materials including paper, polyolefins, oriented polyolefins, polyesters, ionomers, PVC, unplasticized PVC, and other polar polymers. They are made for use as heat seal layer, adhesive layer, or modifier for cost/performance enhancement. They are soft, pliable, and tough at ambient and freezing temperatures and exhibit excellent ESCR. These polymers exhibit high solids fillability and compatibility with a wide range of polymers. This facilitates their use as bases for all-purpose concentrates for addition to a wide spectrum of polymers. They process like LDPE.
Physical Properties Metric English Comments
Density 0.941 g/cc
0.0340 lb/in³
ASTM-D1505
Melt Flow 8.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
8.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM-D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 39
39
ASTM-D2240
Tensile Strength at Break 8.27 MPa
1200 psi
500 mm/min (20 in./min); ASTM-D638 Type IV Specimen
Elongation at Break 600 %
600 %
500 mm/min (20 in./min); ASTM-D638 Type IV Specimen
Thermal Properties Metric English Comments
Melting Point 82.0 °C
180 °F
DSC; ASTM-D3418
Vicat Softening Point 50.0 °C
122 °F
ASTM-D1525
Brittleness Temperature <= -73.0 °C
<= -99.4 °F
ASTM-D746
Descriptive Properties Value Comments
Methyl Acrylate Content (%) 20
Process Extrusion
Region US & Canada
Bamberger Polymers Distribution