Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 60.0 - 70.0 °C | 140 - 158 °F | |
Fine Organics FINALUX G 471 Lubricant Additive Applications: Intermediate lubricant suggested for rigid PVC processing especially extrusion.Information provided by Fine Organics |
|||
Melting Point | 60.0 - 70.0 °C | 140 - 158 °F | MQSA 70 A |
Lubrizol Advanced Materials PEARLBOND® 106 Linear Thermoplastic Polyurethane Pearlbond™ 106.is a linear, aromatic polyurethane, supplied in form of small white or slightly yellowish granules, which combines a high crystallisation rate with a very high thermoplasticity l.. |
|||
Melting Point | 66.0 - 70.0 °C | 151 - 158 °F | MQSA 70 A |
Lubrizol Advanced Materials Pearlbond® 550 Thermoplastic Polyurethane Pearlbond™ 550 is a linear, polycaprolactone-copolyester polyurethane, supplied in form of white spherical granules with a very high crystallization rate and a very high thermoplasticity level... |
|||
Melting Point | 66.0 - 70.0 °C | 151 - 158 °F | MQSA 70 A |
Lubrizol Advanced Materials Pearlbond® D170 Thermoplastic Polyurethane Pearlbond® D170 is a TPU grade designed for use with Heat Sealable Fabrics. This grade is to be applied in thermo bonding (heat-sealing) processes, through which the adhesive is laid on a series.. |
|||
Melting Point | 20.0 - 70.0 °C | 68.0 - 158 °F | |
BASF 3-Hexyne-2,5-diol Formula: C6H10O2OCAS: 3031-66-1Description: 3-Hexyne-2,5-diol is a yellowish liquid or solidified, with a pungent odor. It is miscible in water.Synonyms: Hexin-3-diol-2,5, Hex-3-yne-2,5-diol, Hex-3.. |