Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 7.00 - 8.00 °C | 44.6 - 46.4 °F | |
Indium Corp. Indalloy® 46L Ga-In-Sn-Zn Alloy for Mercury Replacement Alloy liquid at room temperature, wets glass and quartz. Mercury replacement.Information provided by the manufacturer, Indium Corporation. |
|||
Melting Point | <= 7.00 °C | <= 44.6 °F | |
Dow Corning 3225C Formulation Aid Dispersion of high molecular weight silicone surfactant in volatile dimethylsiloxane, designed to prepare water-in-silicone emulsions.Information provided by Dow Corning |
|||
Melting Point | <= 7.00 °C | <= 44.6 °F | |
BASF Benzyl chloroformate Formula: C8H7NCIOCAS: 501-53-1Description: Benzyl chloroformate is a colorless to yellow liquid, with a pungent odor. It spontaneously decomposes as a reaction to water. Synonyms: Chloroformic acid.. |