Polymer Property : Melting Point = 44.6 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 7.00 - 8.00 °C
44.6 - 46.4 °F
Indium Corp. Indalloy® 46L Ga-In-Sn-Zn Alloy for Mercury Replacement
Alloy liquid at room temperature, wets glass and quartz. Mercury replacement.Information provided by the manufacturer, Indium Corporation.
Melting Point <= 7.00 °C
<= 44.6 °F
Dow Corning 3225C Formulation Aid
Dispersion of high molecular weight silicone surfactant in volatile dimethylsiloxane, designed to prepare water-in-silicone emulsions.Information provided by Dow Corning
Melting Point <= 7.00 °C
<= 44.6 °F
BASF Benzyl chloroformate
Formula: C8H7NCIOCAS: 501-53-1Description: Benzyl chloroformate is a colorless to yellow liquid, with a pungent odor. It spontaneously decomposes as a reaction to water. Synonyms: Chloroformic acid..