Polymer Property : Melting Point = 640 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 540 - 640 °C
1000 - 1180 °F
Magnesium Elektron Elektron® 43 Magnesium Wrought Alloy
High strength wrought Mg alloy available as rolled plate, forging feedstock, and extrusions. It is a wrought evolution of the casting alloy Elektron WE43. Elektron 43 uses zirconium grain refining..