Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 540 - 640 °C | 1000 - 1180 °F | |
Magnesium Elektron Elektron® 43 Magnesium Wrought Alloy High strength wrought Mg alloy available as rolled plate, forging feedstock, and extrusions. It is a wrought evolution of the casting alloy Elektron WE43. Elektron 43 uses zirconium grain refining.. |