Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 47.0 - 49.0 °C | 117 - 120 °F | |
Hong Kun Group BP 12 Additive Chemical Name: 2-hydroxy-4-(octyloxy)benzophenoneCAS No. 1843-05-6All information provided by Hongkun Group |
|||
Melting Point | 47.0 - 49.0 °C | 117 - 120 °F | |
Hong Kun Group UV 531 UV Absorber Chemical Name: 2-hydroxy-4-(octyloxy)benzophenoneCAS No. 1843-05-6All information provided by Hongkun Group |
|||
Melting Point | 47.0 - 49.0 °C | 117 - 120 °F | |
M Chemical GUARD DOGâ„¢ UV531 Light Absorber (Flake or Powder), Benzophenone Derivative GUARD DOGâ„¢ UV531(flake or powder) light stabilizer is a derivative of Benzophenone that has an exceptionally strong and broad-range of UV absorption properties (UV A 315 -400 nm and UV B 290 - .. |
|||
Melting Point | 47.0 - 49.0 °C | 117 - 120 °F | |
Suqian Unitechem UV-531 Chemical Name: 2-Hydroxy-4-Octyloxy BenxophenoneCAS NO.: 1843-05-6Properties: Freely soluble in benzene, n-hexane, acetone, slightly soluble in ethanol, very slightly soluble in ethane dichloride.Us.. |