Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 47.0 - 49.0 °C | 117 - 120 °F | |
Hong Kun Group BP 12 Additive Chemical Name: 2-hydroxy-4-(octyloxy)benzophenoneCAS No. 1843-05-6All information provided by Hongkun Group |
|||
Melting Point | 47.0 - 49.0 °C | 117 - 120 °F | |
Hong Kun Group UV 531 UV Absorber Chemical Name: 2-hydroxy-4-(octyloxy)benzophenoneCAS No. 1843-05-6All information provided by Hongkun Group |
|||
Melting Point | 47.0 - 49.0 °C | 117 - 120 °F | |
M Chemical GUARD DOGâ„¢ UV531 Light Absorber (Flake or Powder), Benzophenone Derivative GUARD DOGâ„¢ UV531(flake or powder) light stabilizer is a derivative of Benzophenone that has an exceptionally strong and broad-range of UV absorption properties (UV A 315 -400 nm and UV B 290 - .. |
|||
Melting Point | 47.0 - 52.0 °C | 117 - 126 °F | |
Indium Corp. Indalloy 16 Low Melting Bismuth Alloy Information Provided by Indium Corporation |
|||
Melting Point | 47.0 °C | 117 °F | Eutectic |
Indium Corp. Indalloy® 117 Bi-Pb-In-Sn-Cd Fusible Alloy General purpose fusible alloy.Information provided by the manufacturer, Indium Corporation. |
|||
Melting Point | 47.0 - 57.0 °C | 117 - 135 °F | |
Struktol V-DSP Processing Additive Fatty acid esterTypical Applications: STRUKTOL® V-DSP is a highly compatible, internal PVC lubricant. It is particularly good at improving melt flow thus reducing amperage and head pressure for c.. |
|||
Melting Point | 47.0 - 49.0 °C | 117 - 120 °F | |
Suqian Unitechem UV-531 Chemical Name: 2-Hydroxy-4-Octyloxy BenxophenoneCAS NO.: 1843-05-6Properties: Freely soluble in benzene, n-hexane, acetone, slightly soluble in ethanol, very slightly soluble in ethane dichloride.Us.. |
|||
Melting Point | 47.0 - 88.0 °C | 117 - 190 °F | ASTM D3418(DSC) |
DuPont Surlyn® 8945 Thermoplastic Ionomer Resin Surlyn® 8945 provides high flow properties and consistent, easy processing in molded and extruded applications. It is positioned in the medium/high acid, high neutralization area of the ionomer sp.. |
|||
Melting Point | 47.0 °C | 117 °F | |
AIM 47 Fusible Bismuth Alloy Uses: low-temperature solder; fixturing delicate parts for machining; lens blocking; proof casting of cavities; dental models; fusible element in safety devices and alarms; radiation blocking for x-.. |
|||
Melting Point | 47.0 - 105 °C | 117 - 221 °F | Average value: 84.7 °C Grade Count:40 |
Overview of materials for Ionomer, Molded This property data is a summary of similar materials in the MatWeb database for the category "Ionomer, Molded". Each property range of values reported is minimum and maximum values of appropriate Ma.. |
|||
Melting Point | 47.0 °C | 117 °F | Freezing Point; ASTM D3418 |
DuPont Elvax® CM576 Ethylene Vinyl Acetate
(discontinued **) DuPont™ Elvax® CM576 is an ethylene-vinyl acetate copolymer resin for use in industrial applications. Specialty grades of Elvax® have the unusual combination of high vinyl acetate levels and low .. |
|||
Melting Point | 47.0 °C | 117 °F | Freezing Point; ASTM D3418 |
DuPont Elvax® CM4875 Ethylene Vinyl Acetate
(discontinued **) DuPont™ Elvax® CM4875 is an ethylene-vinyl acetate copolymer resin for use in industrial applications. Specialty grades of Elvax® have the unusual combination of high vinyl acetate levels and low.. |